A deodorant and additive technology, which is applied in solvent extraction, solid solvent extraction, gas treatment, etc., can solve the problems of low efficiency, long removal time, and low formaldehyde purification and removal effect, so as to improve the absorption and purification rate and reduce the The content of benzene, the effect of improving the removal and purification effect
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Image
Examples
preparation example Construction
[0026] A preparation method of deodorant, comprising the following steps:
[0027] S1. Add the carrier resin, adsorption additives, nano-anion powder and water together into the stirring pot, and then slowly add sodium benzoate, adipic dihydrazide, guanidine hydrochloride, sodium metabisulfite and essence at a speed of 450-650r / min ;
[0028] S2. After all the raw materials in S1 are stirred evenly, continue to add Adiantum extract and formaldehyde purification solution therein, and then continue to stir for 30 to 45 minutes. After the end, a mixture is obtained;
[0029] S3. Put the mixture into parallel twin-screw extruders and extrude it. After cooling and drying in a water bath and cold air, send it to a granulator and discharge it from the discharge port to obtain a granular deodorant.
[0030] Wherein, the extruding temperature parameter of the extruder is controlled between 100-1200° C., and the particle diameter of the prepared deodorant is between 1.5-3.5 cm.
Embodiment 1
[0032] A deodorant, comprising the following raw materials by mass percentage: carrier resin 15%, sodium benzoate 1.5%, adipic acid dihydrazide 2.0%, guanidine hydrochloride 0.3%, sodium pyrosulfite 1.5%, activated carbon 5.0%, zeolite 5.0% , 5.0% bentonite, 3.0% essence, 3.5% formaldehyde purification solution, 3.5% maidenhair fern extract, 3.5% nano negative ion powder, and the rest is water.
Embodiment 2
[0034] A deodorant, comprising the following raw materials in terms of mass percentage: carrier resin 18%, sodium benzoate 1.7%, adipic acid dihydrazide 2.3%, guanidine hydrochloride 0.5%, sodium pyrosulfite 1.7%, activated carbon 7.5%, zeolite 7.5% , 7.5% bentonite, 3.3% essence, 5.2% formaldehyde purification solution, 4.0% maidenhair fern extract, 3.8% nano negative ion powder, and the rest is water.
PUM
| Property | Measurement | Unit |
|---|---|---|
| Particle size | aaaaa | aaaaa |
Abstract
Description
Claims
Application Information
Login to View More - R&D
- Intellectual Property
- Life Sciences
- Materials
- Tech Scout
- Unparalleled Data Quality
- Higher Quality Content
- 60% Fewer Hallucinations
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2025 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com