Hydrocolloid medical dressing and preparation method thereof
A hydrocolloid and raw material technology, applied in medical science, bandages, absorbent pads, etc., can solve the problems of inability to promote wound healing, wound mechanical damage, poor protection effect, etc.
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Examples
preparation example Construction
[0015] The embodiment of the present invention provides a method for preparing a hydrocolloid medical dressing, which includes the following steps: taking SIS block copolymer, polyisobutylene, rosin glyceride and antioxidant and mixing them in an internal mixer to prepare a hot-melt pressed dressing Sensitive glue; add hydrocolloid particles to the above hot melt pressure sensitive adhesive, continue mixing to obtain a mixture; place the mixture in a flat vulcanizer to prepare a finished hydrocolloid dressing; wherein, the above hydrocolloid particles include carboxymethyl cellulose Sodium, polyvinyl alcohol and sodium alginate.
[0016] In the above-mentioned embodiment, firstly, the SIS block copolymer, polyisobutylene, rosin glyceride and antioxidant were mixed in an internal mixer to prepare a hot-melt pressure-sensitive adhesive, and the hot-melt pressure-sensitive adhesive was used as the base material. Among them, the SIS block copolymer is a triblock copolymer of styre...
Embodiment 1
[0037] The present embodiment provides a hydrocolloid medical dressing, which is prepared by the following method:
[0038] Take 10g of SIS block copolymer, 12g of polyisobutylene, 15g of rosin glyceride and 0.2g of antioxidant and put them into an internal mixer and mix them for 15min at 120°C and 100r / min to prepare a hot-melt pressure-sensitive adhesive; Add hydrocolloid particles to the hot-melt pressure-sensitive adhesive, keep the temperature and rotation speed constant, and continue mixing for 15 minutes to obtain a mixture, wherein the raw materials of the hydrocolloid particles include 30 g of sodium carboxymethyl cellulose, 10 g of polyvinyl alcohol and 8 g of sodium alginate Add foaming agent to the mixture, cool after stirring and mixing, and then place it in a flat vulcanizer to prepare the finished hydrocolloid dressing; wherein, the amount of foaming agent is 5% of the weight of the above-mentioned mixture, and the raw material of foaming agent includes carbonic ...
Embodiment 2
[0040] The present embodiment provides a hydrocolloid medical dressing, which is prepared by the following method:
[0041] Take 20g of SIS block copolymer, 12g of polyisobutylene, 15g of rosin glyceride and 0.8g of antioxidant, put them into an internal mixer and mix them for 15min at 130°C and 110r / min to prepare a hot-melt pressure-sensitive adhesive; Add hydrocolloid particles to the hot-melt pressure-sensitive adhesive, keep the temperature and rotation speed constant, and continue mixing for 15 minutes to obtain a mixture, wherein the raw materials of the hydrocolloid particles include 35 g of sodium carboxymethyl cellulose, 10 g of polyvinyl alcohol and 12 g of sodium alginate Add foaming agent to the mixture, cool after stirring and mixing, and then place it in a flat vulcanizer to prepare the finished hydrocolloid dressing; wherein, the amount of foaming agent is 7% of the weight of the above-mentioned mixture, and the raw material of foaming agent includes carbonic ac...
PUM
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com