Solar cell frame material and preparation method thereof
A solar cell and frame technology, applied in the field of materials, can solve the problems of unenvironmental protection, unfriendly glass fiber reinforced plastic manufacturing environment, and large waste.
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Image
Examples
Embodiment 1
[0033] CBT: catalyst: poly-p-phenylene benzobisoxazole fiber: diphenylamine: p-phenylenediamine = 29%: 0.12%: 70.5%: 0.18%: 0.2%; mold temperature: 185°C;
[0034] Impregnation of polyparaphenylene benzobisoxazole fibers in CBT and Ti(OCH) 2 CH 3 ) 4 In the mixture of , diphenylamine and p-phenylenediamine, the pre-impregnated material is passed through a mold with a temperature of 185 ° C, and the cross-section of the mold has the same cross-section as the solar cell frame. Through continuous extrusion and pultrusion, a profile with a regular interface is obtained. The profile is cut, screwed, and bonded with adhesive to obtain a frame structure product.
Embodiment 2
[0036] CBT: catalyst: carbon fiber: diphenylamine: p-phenylenediamine = 29%: 0.13%: 70.5%: 0.17%: 0.2%; mold temperature: 185°C;
[0037] Impregnating carbon fibers in CBT and Ti(OCH 2 CH 3 ) 4 In the mixture of , diphenylamine and p-phenylenediamine, the pre-impregnated material is passed through a mold with a temperature of 185 ° C, and the cross-section of the mold has the same cross-section as the solar cell frame. Through continuous extrusion and pultrusion, a profile with a regular interface is obtained. The profile is cut, screwed, and bonded with adhesive to obtain a frame structure product.
Embodiment 3
[0039] CBT: catalyst: glass fiber: diphenylamine: p-phenylenediamine = 29%: 0.12%: 70.5%: 0.18%: 0.2%; mold temperature: 185°C;
[0040] Impregnating glass fibers in CBT and Ti(OCH 2 CH 3 ) 4 In the mixture of , diphenylamine and p-phenylenediamine, the pre-impregnated material is passed through a mold with a temperature of 185 ° C, and the cross-section of the mold has the end of a solar cell frame. Through continuous extrusion and pultrusion, a profile with a regular interface is obtained. The profile is cut, screwed, and bonded with adhesive to obtain a frame structure product.
PUM
| Property | Measurement | Unit |
|---|---|---|
| density | aaaaa | aaaaa |
| density | aaaaa | aaaaa |
| density | aaaaa | aaaaa |