Fiber modified by Chinese traditional medicine and manufacturing method thereof
A technology for modifying fibers and manufacturing methods, which is applied in rayon manufacturing, fiber chemical characteristics, textiles and papermaking, etc. It can solve the problems of too simple methods, loss of drug properties, and textile properties such as hard hand feeling, etc., and achieve simple processing routes , Ease of industrial production
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Examples
Embodiment 1
[0031] The selected medicine Qianjinzi is used as a raw material, and Qianjinzi has inhibitory effects on bacteria such as Glucobacterium aureus, Escherichia coli, and Pseudomonas aeruginosa. Production of traditional Chinese medicine modified polyacrylonitrile fiber containing 5 parts of stephenia superfine powder and 95 parts of polyacrylonitrile.
[0032] Pulverize Qianjinzi, and then use ultrafine powder processing equipment to process it into an ultrafine powder with an average particle size of <5 microns, add 0.5% of the Caustic soda solution, and disperse with ultrasonic waves at room temperature for 30 minutes to form a uniformly dispersed emulsion to make a uniformly dispersed emulsion, add the emulsion to the spinning stock solution containing 92 parts of polyacrylonitrile for blending, and then stir and defoam After 6 hours, according to the wet spinning process route, the modified acrylic fiber of Qianjinzi was processed, and the fiber had certain antibacterial pro...
Embodiment 2
[0034] Take a prescription that can disinfect and relieve itching as an example. Production of traditional Chinese medicine modified viscose fiber containing 10 parts of traditional Chinese medicine ultrafine powder and 90 parts of viscose cellulose.
[0035] Choose 3.5 parts of Sophora flavescens, 2 parts of Verbena, 1.0 part of Dandelion, 0.5 part of Cnidium, 0.5 part of Galla, 1.5 parts of Pepper, 0.5 part of Zanthoxylum bungeanum, and 0.5 part of Alum. Ultrafine powder with an average particle size of <5 microns, then sequentially added to 0.5% caustic soda solution, ultrasonically dispersed at room temperature, stirred evenly, and then the mixed emulsion was added to the river bank with 90 parts of viscose cellulose Spinning stock solution, then stirred and defoamed for 4 hours, processed according to the wet spinning process to make traditional Chinese medicine modified viscose fiber, the fiber has certain disinfection and antipruritic properties, and can be made into un...
PUM
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com