A running board and self-lubricating technology, which is applied in the direction of sports accessories, layered products, synthetic resin layered products, etc., can solve the problems of burning instruments or control lines, separation layers, troubles, etc., and achieve the effect of improving anti-static interference ability
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Examples
Embodiment 1
[0040] This self-lubricating running board is directly poured and solidified to form a self-lubricating layer on the surface of the hard floor MDF. The manufacturing method is:
[0041] (1) The chemical composition (by weight) of the self-lubricating layer is:
[0042] Unsaturated polyester resin 100, initiator (methyl ethyl ketone peroxide) 2.0, accelerator (10% concentration of cobalt peroxide stearate) 1.0, diluent (styrene) 15.0, lubricant 5.0,
[0043] The lubricant is 10% molybdenum disulfide (MoS 2 ) and 20% tungsten disulfide (WS 2 ) of diethylene glycol (CH 2 OH·CH 2 O·CH 2 CH 2 OH) dispersion, its preparation method is: 7Kg diethylene glycol, add 1Kg molybdenum disulfide and 2Kg tungsten disulfide, grind with sand mill for 5 hours and disperse.
[0044] (2) Process steps
[0045] (i) The temperature at the construction site: 5°C, the curing time is 16 minutes, and the friction coefficient is selected as 0.11.
[0046] (ii) Compound preparation
[0047] ① Selec...
Embodiment 2
[0053] This self-lubricating running board is bonded with a layer of foam elastic layer on the plywood of the hard floor, and directly casts and solidifies a layer of self-lubricating layer on the elastic layer. The manufacturing method is as follows:
[0054] (1) The chemical composition (by weight) of the self-lubricating layer is:
[0055] Unsaturated polyester resin 100, initiator (methyl ethyl ketone peroxide) 1.0, accelerator (cobalt peroxystearate of 10% concentration) 0.6, diluent (styrene) 5.0, lubricant (preparation method with example 1) 5.0 ,
[0056] (2) Process steps
[0057] (i) The temperature at the construction site is 25°C, the curing time is 12 minutes, and the friction coefficient is selected as 0.11.
[0058] The following steps are the same as in Example 1.
Embodiment 3
[0060] The self-lubricating running board is directly poured and solidified on the plywood surface of the hard base to form a self-lubricating layer. The manufacturing method is:
[0061] (1) The chemical composition (by weight) of the self-lubricating layer is:
[0062] Unsaturated polyester resin 100, initiator (methyl ethyl ketone peroxide) 0.8, accelerator (cobalt peroxystearate of 10% concentration) 0.4, diluent (styrene) 0, lubricant (preparation method with example 1) 5.0 ,
[0063] (2) Process steps
[0064] (i) The temperature at the construction site is 38°C, the curing time is 8 minutes, and the friction coefficient is selected as 0.10.
[0065] The following steps are the same as in Example 1.
PUM
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com