Dipping glue for papreg and preparing method thereof
A production method and technology of impregnating glue, applied in the direction of cellulose plastic layered products, layered products, chemical instruments and methods, etc., can solve the problems of not providing the production method of melamine glue, etc.
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Image
Examples
Embodiment 1
[0010] Embodiment 1 (referring to the proportioning figure of parts by weight in the above table):
[0011] First, add 400 parts by weight of nonylphenol (if phenol is used, it needs to be melted first) and 600 parts by weight of furfural into the reactor for stirring, add about 8 parts by weight of NaoH to adjust the pH value to 8.0-9.5, and then evenly heat up to 40-45°C , add 300 parts by weight of melamine and continue to heat up, but the heating rate needs to be controlled, and the temperature should be kept at 90-95°C, and the pH value should be measured and controlled. When the water temperature is 20°C, the water-soluble ratio reaches 1-0.7 times or the turbidity test has spherical objects, and the reaction has reached the end. During the process, the reaction is kept for 45-60 minutes, and the temperature is immediately lowered, and 650 parts by weight of ethanol is added, and the temperature is lowered to 45°C. The feeding is over.
[0012] Examples 2-10 The dipping...