[0008] The preparation method of the present invention is the following steps:
[0009] Before weaving, the spandex covering yarn first performs thermal fixed type, the set temperature is 65-70 ° C, the insulation time is 15-20min, and the exhaust time is 2min. Starch slurry, in which the slurry formula is used: 50kg of variability starch, 25kg of acrylin, LMA-985.5kg, S-52D 3kg, table meridian slurry formula: PVA179925kg, oxidized starch 40kg, methyl esters 25kg 25kg material , P-T 3kg, S-52D 3kg, 0.25kg emulsifier, 95 ° C in the slurry grooves, 10-45m / min, the inner layer of the fabric uses Fang Ping tissue, the outer layer is the honeycomb tissue structure. The latitude yarn is covered with 30s cotton amino ammonia, and the table is 32S color cotton and fast -drying wet fiber covering yarn. Weft density: 146 pieces / inch, width: 63 inches, the warp ratio of the inside and the outside is 1:2, and the stitching point organization is warp weight flat.
Embodiment 1
[0012] Ingredients: Weisha 30s cotton amino ammonia covered yarn, table scriptures are: 32S color cotton and fast dry wet fibers cover the yarn, the mix is: 21S cotton and far -infrared functional fiber spinning yarn;
[0013] Preparation:
[0014] Before weaving, the spandex covering yarn first performs thermal fixed type, the set temperature is 65-70 ° C, the insulation time is 15-20min, and the exhaust time is 2min. Starch slurry, in which the slurry formula is used: 50kg of variability starch, 25kg of acrylics, LMA-985.5kg, S-52D 3kg, table meridian slurry formula: PVA1799 25kg, oxidized starch 40kg, methyl ester paste material 25kg, P-T 3kg, S-52D 3kg, emulsifier 0.25kg, sizing tank temperature 95℃, sizing speed 30-45m / min, the inner layer of the fabric adopts a square weave, and the outer layer is a honeycomb structure. Layer weft yarns are 30s cotton spandex covered yarn, surface warp is 32s colored cotton and fast-drying moisture-wicking fiber covered yarn, inner warp...
Embodiment 2
[0016] Ingredients: weft yarn 30s cotton spandex covered yarn, inner warp: 32s colored cotton and fast-drying moisture-conducting fiber covered yarn, surface warp: 21s cotton and far-infrared functional fiber blended yarn, the preparation method is the same as that in Example 1.
[0017] To sum up, the elastic honeycomb double-layer fabric of the present invention uses cotton spandex covered yarns as weft yarns, and warp yarns use blended yarns or covered yarns with moisture-conducting function and far-infrared function. The layered honeycomb structure has a stronger three-dimensional effect under the action of elastic shrinkage. At the same time, the double-layer structure and far-infrared functional fibers are used to improve the overall thermal insulation effect of the fabric and improve the production value of the product.
PUM
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com