A technology of non-chromium metal and compound tanning agent, which is applied in the field of chrome-free tanning of cattle upper leather, can solve the problems of leather shrinkage temperature not being stable above 85℃, low shrinkage temperature, poor processability, etc. Industrial production base, good matching, and the effect of promoting distribution

Inactive Publication Date: 2009-02-25
WENZHOU UNIVERSITY
View PDF0 Cites 2 Cited by
  • Summary
  • Abstract
  • Description
  • Claims
  • Application Information

AI Technical Summary

Problems solved by technology

These three technologies have one or more of the following problems in the actual industrial production engineering: the shrinkage temperature of leather cannot be stabilized above 85°C; the performance of leather is far behind that of chrome-tanned leather; Some leather processing technology systems; the elimination of chromium pollution brings pollution problems such as organic phosphorus and formaldehyde
[0004] In addition, the common chrome-free tanned leather often has insufficient whiteness when producing shoe upper leather products; or it is not resistant to yellowing; the shrinkage temperature is not high, which is not conducive to subsequent processing and shoemaking processing.

Method used

the structure of the environmentally friendly knitted fabric provided by the present invention; figure 2 Flow chart of the yarn wrapping machine for environmentally friendly knitted fabrics and storage devices; image 3 Is the parameter map of the yarn covering machine
View more

Examples

Experimental program
Comparison scheme
Effect test

Embodiment 1

[0047] (1) Pretreatment: conventional caustic soda pickling cowhide is weighed, placed in the drum, the weight of the hide is increased to 200%, and the weight of the material in the drum is 100 parts; 80 parts of Baume degree normal temperature brine, adjust the pH to 2.5; add 0.3 parts of non-ionic oil, and rotate for 20 minutes; add 0.8 parts of pretreatment agent AT-6, and rotate for 30 minutes;

[0048] (2) Tanning: add 8 parts of non-chrome metal compound tanning agent, 1.3 parts of chrome-free tanning partner D5, and rotate for 120 minutes; add 0.7 parts of sharp tanning agent GM-15, and rotate for 180 minutes; The pH is 3.5; finally add 100 parts of hot water at 60°C, keep the internal temperature at 36°C, and rotate for 60 minutes; overnight, wash the drum out with water the next day.

Embodiment 2

[0050] (1) Pretreatment: conventional caustic soda pickling cowhide is weighed, placed in the drum, the weight of the hide is increased to 200%, and the weight of the material in the drum is 100 parts; 80 parts of Baume degree normal temperature brine, adjust the pH to 2.5; add 0.3 parts of non-ionic oil, and rotate for 20 minutes; add 0.8 parts of pretreatment agent AT-6, and rotate for 30 minutes;

[0051](2) Tanning: add 14 parts of non-chrome metal compound tanning agent, 3.3 parts of chrome-free tanning partner D5, and rotate for 150 minutes; add 1.6 parts of sharp tanning agent GM-15, and rotate for 150 minutes; The pH is 3.6; finally add 120 parts of hot water at 60°C, keep the internal temperature at 37°C, and rotate for 60 minutes; overnight, wash out the drum with water the next day.

Embodiment 3

[0053] (1) Pretreatment: conventional caustic soda pickling cowhide is weighed, placed in the drum, the weight of the hide is increased to 200%, and the weight of the material in the drum is 100 parts; 80 parts of Baume degree normal temperature brine, adjust the pH to 2.5; add 0.3 parts of non-ionic oil, and rotate for 20 minutes; add 0.8 parts of pretreatment agent AT-6, and rotate for 30 minutes;

[0054] (2) Tanning: add 20 parts of non-chrome metal compound tanning agent, 5.0 parts of chrome-free tanning companion D5, and rotate for 180 minutes; add 2.5 parts of sharp tanning agent GM-15, and rotate for 120 minutes; The pH is 3.7; finally add 150 parts of hot water at 60°C, keep the internal temperature at 38°C, and rotate for 60 minutes; overnight, wash out the drum with water the next day.

the structure of the environmentally friendly knitted fabric provided by the present invention; figure 2 Flow chart of the yarn wrapping machine for environmentally friendly knitted fabrics and storage devices; image 3 Is the parameter map of the yarn covering machine
Login to view more

PUM

PropertyMeasurementUnit
temperatureaaaaaaaaaa
Login to view more

Abstract

The invention relates to a method of tanning cattle shoe upper leather with non-chrome metal compound tanning agent, comprising steps of pre-treatment, tanning and after-treatment. LTA-100 metal (chrome-free) compound tanning agent, chrome-free tanning partner D5, tanning assisting agent GM-15 and the like are adopted during the process of tanning. The invention is characterized in that: the shrinkage temperature of leather in the industrialized production can be stabilized above 85 DEG C, even above 90 DEG C; chrome pollution and phosphorus pollution are not produced, and formaldehyde is not released; the dyeing color is so rich that the color is better for white rather than that of the chrome tanning leather; the tannery sludge can be directly burned without causing potential danger of hexavalent chrome. The invention can be sued for substituting the traditional technique of leather tanning by chrome powder, meanwhile eliminating pollution to humankind and environment by chromium salts during the process and in the wastes of leather products. The productobtained by the method has good strength, thus blazing a trail in producing chrome-free tanning cattle shoe upper leather for tanneries.

Description

technical field [0001] The invention belongs to the field of leather tanning, and in particular relates to a chrome-free tanning technology of yellow cow shoe upper leather. Background technique [0002] Chrome tanning, which has a history of more than 100 years, has been the mainstream technology of leather tanning because it can impart excellent performance to leather, and it is almost unshakable. Chromium pollution in the tanning industry has three sources: first, pollution in the production and processing of chromium-containing materials; second, pollution in sewage, sludge, and chromium-containing solid waste in the tanning production process; Third, secondary pollution to the environment after consumption of chromium-containing products. This pollution is often ignored by people, but it accounts for about 70% of the total chromium pollution in the whole leather industry, and it is quite scattered, which is not conducive to treatment or recovery. With the development ...

Claims

the structure of the environmentally friendly knitted fabric provided by the present invention; figure 2 Flow chart of the yarn wrapping machine for environmentally friendly knitted fabrics and storage devices; image 3 Is the parameter map of the yarn covering machine
Login to view more

Application Information

Patent Timeline
no application Login to view more
Patent Type & Authority Applications(China)
IPC IPC(8): C14C3/02
Inventor 兰云军周建飞刘建国柴玉叶
Owner WENZHOU UNIVERSITY
Who we serve
  • R&D Engineer
  • R&D Manager
  • IP Professional
Why Eureka
  • Industry Leading Data Capabilities
  • Powerful AI technology
  • Patent DNA Extraction
Social media
Try Eureka
PatSnap group products