Conditioning deodorization antibiotic mildew-proof wallpaper
An antibacterial, mildew proof and humidity control technology, applied in the field of building decoration materials
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Examples
Embodiment 1
[0014] The wallpaper of the present invention is 90g / m 2 The base paper is used as the carrier, and the paste paste is coated on the base paper carrier. After drying and gelling, it is cooled and printed. The paste is made by weight percentage: PVC33%, sepiolite and 45.5% of zeolite mixture, of which 25.5% of sepiolite, 20% of zeolite, 10% of titanium dioxide, 3% of nano-ZnO, nano-TiO 2 1%, ZOE 2%, 1,2-dicarboxydiisononyl ester 2%, TXIB viscosity reducer 1.0%, octyl tin mercaptan (T890) 2% and bisphenol A 0.5%, first make PVC Mix the paste with bisphenol A and plasticizer and mix well, then add sepiolite and zeolite mixture, or attapulgite and zeolite mixture and mix well, then add titanium dioxide, nano-ZnO, nano-TiO 2 After mixing with antifungal agent, dispersing and stirring, add stabilizer, mix and stir evenly, and finally add viscosity reducer to adjust viscosity to make overcoating paste, each 900g / m 2 The base paper is recoated with 100g of slurry paste, dried and gelatini...
Embodiment 2
[0020] The wallpaper of the present invention is 90g / m 2 The base paper is used as the carrier, and the paste paste is coated on the base paper carrier. After drying and gelatinization, it is cooled and printed. The paste is made by weight percentage: PVC28%, attapulgite And zeolite mixture 45.5%, including attapulgite 25.5%, zeolite 20%, titanium dioxide 15%, nano-ZnO 2%, nano-TiO 2 2%, ZOE 2%, 1,2-dicarboxydiisononyl ester 2%, TXIB viscosity reducer 1.0%, octyl tin mercaptan (T890) 2% and bisphenol A 0.5%, first make PVC Mix the paste with bisphenol A and plasticizer and mix well, then add sepiolite and zeolite mixture, or attapulgite and zeolite mixture and mix well, then add titanium dioxide, nano-ZnO, nano-TiO 2 After mixing with anti-mold agent, dispersing and stirring, add stabilizer, mix and stir evenly, and finally add viscosity reducer to adjust viscosity to make overcoating paste, every 90g / m 2 The base paper is recoated with 100g of slurry paste, dried and gelatinized,...
Embodiment 3
[0026] The wallpaper of the present invention is 80g / m 2 The base paper is used as the carrier, and the paste paste is coated on the base paper carrier. After drying and gelling, it is cooled and printed. The paste is made by weight percentage: PVC40%, attapulgite And zeolite mixture 35%, including attapulgite 20%, zeolite 15%, titanium dioxide 13.5%, nano-ZnO 2%, nano-TiO 2 2%, ZOE 2%, 1,2-dicarboxydiisononyl ester 2%, TXIB viscosity reducer 1.0%, octyl tin mercaptan (T890) 2%, and bisphenol A 0.5%. First, make PVC Mix the paste with bisphenol A and plasticizer and stir evenly, then add sepiolite and zeolite mixture, or attapulgite and zeolite mixture and mix well, then add titanium dioxide, nano ZnO, nano TiO 2 After mixing with anti-mold agent, dispersing and stirring, add stabilizer, mix and stir evenly, and finally add viscosity reducer to adjust the viscosity to make overcoating paste, every 80g / m 2 The base paper is recoated with 100g of slurry paste, dried and gelatinized,...
PUM
Property | Measurement | Unit |
---|---|---|
Particle size | aaaaa | aaaaa |
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com