A polyester low-elasticity and production method technology, which is applied in dyeing, heating/cooling fabrics, textiles and papermaking, etc., can solve the problems of high manufacturing cost, itchy feeling of close-fitting bedding, high cost, etc., to meet the market pursuit and reasonable process Efficient, short production cycle results
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Examples
Embodiment 1
[0029] Warp knitted polyester dyed carpet, finished product width 150cm, weight 1000g / m 2 Its production steps are:
[0030] (1) Raw material preparation, selection and preparation of raw materials, use 600D / 192F (3.13D) polyester low-elasticity network yarn as the raw material of velvet yarn, 150D / 48F polyester full-drawn yarn as the base yarn, of which 600D / 192F polyester low-elasticity network Silk accounted for 80%, 150D / 48F polyester fully drawn silk 20%, the stated percentage is the mass percentage
[0031] (2) Double-needle bed Raschel warp knitting machine is used for weaving, and the weight of gray cloth is 1000g / m 2 , width 150cm
[0032] (3) section width;
[0033] (4) Heat setting, the temperature is 200°C, and the fiber heating time is 50 seconds;
[0034] (5) Dyeing, the dye formula is: disperse yellow 0.2g / L, disperse blue 0.2g / L, disperse red 0.8g / L, glacial acetic acid 0.9g / L, high temperature and high pressure 1011 leveling agent 0.25g / L, at 30 Add the d...
Embodiment 2
[0039] Warp knitted polyester printed carpet, finished product width 150cm, weight 1000g / m 2 Its production steps are:
[0040] (1) Raw material preparation, selection and preparation of raw materials, use 600D / 192F (3.13D) polyester low-elasticity network yarn as the raw material of velvet yarn, 150D / 48F polyester full-drawn yarn as the base yarn, of which 600D / 192F polyester low-elasticity network Silk accounted for 80%, 150D / 48F polyester fully drawn silk 20%, the stated percentage is the mass percentage
[0041] (2) Double-needle bed Raschel warp knitting machine is used for weaving, and the weight of gray cloth is 1000g / m 2 , width 150cm
[0042] (3) section width;
[0043] (4) Heat setting, the temperature is 200°C, and the fiber heating time is 50 seconds;
[0044] (5) Printing, the printing formula is: Disperse Red 2g / L, Disperse Yellow 0.8g / L, Disperse Blue 0.2g / L, Sulfuran 8g / L, Urea 20g / L, Plant Paste 30g / L, Thickener 30g / L, made into printing paste, deprinted,...
PUM
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com