Nanometer glass heat-insulating film and manufacturing method thereof
A thermal insulation and nano-scale technology, applied in coatings, polyurea/polyurethane coatings, etc., can solve problems such as environmental protection construction, and achieve the effects of simple and easy construction, cost reduction, and environmentally safe production
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Examples
Embodiment 1
[0032] Pour 400 grams of water into the No. 1 beaker of 1000 milliliters, stir with a magnetic stirrer, the rotating speed is 300rpm, add 10 grams of polycarboxylate sodium salt successively, add 200 grams of nano silicon dioxide, 300 grams of nano titanium dioxide, nano oxide Tin 90 grams, high-speed dispersion, rotating speed is 700rpm; After dispersing for 40 minutes, add to the sand mill, the filling of grinding beads is 50%, carry out sand grinding for 24 hours, pour it out for later use. The nanoacrylic acid emulsion of 300 grams is poured in No. 2 beakers, stirs with magnetic stirrer, and rotating speed is 200rpm, pours 600 grams of nanometer dispersion liquids in No. 1 beakers into No. 2 beakers, then adds 20 grams of ethylene glycol successively, 10 grams of Rohm and Haas 2020, 30 grams of Haichuan Chemical 822, 30 grams of Rohm and Haas RM12W leveling modifier. Increase the speed of the agitator to 600 rpm, and stir for 120 minutes to obtain the nano-glass thermal in...
Embodiment 2
[0034] Pour 700 grams of water into a 1000 ml No. 3 beaker, stir with a magnetic stirrer at a speed of 300 rpm, add 20 grams of polymethacrylic acid in turn, add 50 grams of nano-silica, 100 grams of nano-zinc oxide, and 150 grams of aluminum, high-speed dispersion, rotating speed is 600rpm; after dispersing for 20 minutes, add in the sand mill, the filling of grinding beads is 60%, carry out sand grinding for 24 hours, pour it out for later use. Pour 600 grams of nano-organic silicon-modified acrylic emulsion into No. 4 beaker, stir with a magnetic stirrer at a speed of 200 rpm, pour 300 grams of nano-dispersion in No. 3 beaker into No. 2 beaker, and then add 50 grams Mixture of water and diethylene glycol butyl ether, 10 grams of Rohm and Haas 2020, 20 grams of Haichuan Chemical 822, 20 grams of Rohm and Haas RM12W leveling modifier. Increase the speed of the agitator to 600 rpm, and stir for 120 minutes to obtain the nano-glass thermal insulation coating.
PUM
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com