AdBlue composition as reducing agent for diesel engine with SCR technology
A diesel engine and composition technology, which is applied in the field of special reducing agent - adding blue, can solve the problems of inability to guarantee emission standards, high impurity content, poor stability of the reducing agent, etc., and achieves high oxidation-reduction performance, low impurity content, and high performance. stable effect
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Image
Examples
Embodiment 1
[0021] One, high-purity urea production process comprises the following steps (by weight parts of each component):
[0022] The first step is to put 200-800 parts by weight of pure water into the dissolution kettle, start stirring, and put in 10-40 parts by weight of 3A activated carbon adsorbent; add high-grade industrial urea, pure water and high-grade industrial The ratio of urea is 1:1-4; open the steam valve to heat up, the heating time is 30-40 minutes, and the material is heated to 90-100°C; keep warm at 90-100°C for 20-50 minutes; after the heat preservation is completed, filter the material to the crystallization tank, cooled and crystallized, and vacuum centrifuged and dried for later use.
[0023] In the second step, pure water is put into the dissolution kettle according to the weight of 200-600 parts, and stirring is started; the recrystallized and dried urea in the first step is added, and the ratio of pure water to recrystallized and dried urea is 1:1-4; open th...
Embodiment 2
[0027] One, high-purity urea production process comprises the following steps (by weight parts of each component):
[0028] (1) 400 parts by weight of pure water are dropped into the dissolving kettle, start stirring, and drop into 20 parts by weight of 3A activated carbon adsorbent;
[0029] (2) add industrial urea by weight 1000;
[0030] (3) Open the steam valve to heat up, the heating time is 30-40 minutes, and the material is heated to 90-100°C;
[0031] (4) Insulate at 90-100°C for 30 minutes;
[0032] (5) After the heat preservation is completed, the material is filtered into the crystallization kettle, cooled and crystallized, and vacuum centrifugal drying is carried out simultaneously;
[0033] (6) Pure water is dropped into dissolution kettle by 300 parts by weight, and starts to stir;
[0034] (7) add (5) recrystallized and dried urea by weight 1000;
[0035] (8) Open the steam valve to heat up, the heating time is 30-40 minutes, and the material is heated to 90...
Embodiment 3
[0047] One, high-purity urea production process comprises the following steps (by weight parts of each component):
[0048] (1) 400 parts by weight of pure water are dropped into the dissolving kettle, start stirring, and drop into 20 parts by weight of 3A activated carbon adsorbent;
[0049] (2) add industrial urea by weight 1000;
[0050] (3) Open the steam valve to heat up, the heating time is 30-40 minutes, and the material is heated to 90-100°C;
[0051] (4) Keep warm for 30 minutes at 100±2°C;
[0052] (5) After the heat preservation is completed, the material is filtered into the crystallization kettle, cooled and crystallized, and vacuum centrifugal drying is carried out simultaneously;
[0053] (6) Pure water is dropped into dissolving kettle by weight 300, starts to stir;
[0054] (7) add (5) recrystallized and dried urea by weight 1000;
[0055] (8) Open the steam valve to heat up, the heating time is 30-40 minutes, and the material is heated to 90-100°C;
[00...