Method to prepare full-body tiles by iron tailings
A technology for iron tailings and full-body bricks is applied in the field of comprehensive utilization of building materials and resources, which can solve the problems of consuming high-quality mineral resources, consuming a lot of energy, and low consumption of tailings, and improving the safety factor of mines, and the process is simple and significant. The effect of economic and social benefits
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Image
Examples
Embodiment 1
[0028] as per figure 1 As shown in the technological process, the weight ratio of ingredients is 98.4% of iron tailings, MnO 2 1.6%, after a series of processes such as ball milling, sieving to remove iron, magnetic material enrichment, mud homogenization, spray drying, sieving, powder aging, pressing and drying, it can be made at 1180°C for ten minutes The black full-body brick product has been tested and found to have a water absorption rate of 0.30% and a modulus of rupture of 55MPa.
Embodiment 2
[0030] as per figure 1 As shown in the technological process, the weight ratio of ingredients is 98.4% of iron tailings, MnO 2 0.8%, Cr 2 o 3 0.8%, after a series of processes such as ball milling, sieving to remove iron, magnetic material enrichment, mud homogenization, spray drying, sieving, powder aging, pressing and drying, it can be made at 1180°C for ten minutes The black full-body brick product has been tested and found to have a water absorption rate of 0.42% and a modulus of rupture of 58MPa.
Embodiment 3
[0032] as per figure 1 As shown in the process flow, the weight ratio of ingredients is 96.48% of iron tailings, CuO1.22%, Cr 2 o 3 1.73%, NiO0.57%, after a series of processes such as ball milling, sieving to remove iron, magnetic material enrichment, mud homogenization, spray drying, sieving, powder aging, pressing and drying, etc., heat preservation at 1180 ° C for ten years It can be made into a black full-body brick product in minutes. After testing, the product has a water absorption rate of 0.21% and a modulus of rupture of 51MPa.
PUM
Property | Measurement | Unit |
---|---|---|
modulus | aaaaa | aaaaa |
modulus | aaaaa | aaaaa |
modulus | aaaaa | aaaaa |
Abstract
Description
Claims
Application Information

- Generate Ideas
- Intellectual Property
- Life Sciences
- Materials
- Tech Scout
- Unparalleled Data Quality
- Higher Quality Content
- 60% Fewer Hallucinations
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2025 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com