Architectural porcelain imitating coating
A technology of imitation porcelain paint and paint, applied in the direction of coating, etc., can solve the problems of poor whiteness of paint, easy precipitation and agglomeration, and inability to construct, and achieve the effect of good stain resistance, high hardness, and low cost
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Examples
Embodiment
[0011] A kind of architectural imitation porcelain paint, comprises paint base material glue and gray calcium powder, ground calcium carbonate, ultramarine blue (preparation aqueous solution), tributyl phosphate, and described paint base material glue preferred formula (weight part) is: polyvinyl alcohol (99%) 22-24, formalin water (37%~40%) 12-14, hydrochloric acid 37%~38%) 2-3, sodium hydroxide (solid) 10% aqueous solution 1-3, borax 0.03~0.04, Aluminum ammonium sulfate 0.3-0.4, urea 8-13, tap water 300-600.
[0012] A kind of method for preparing a kind of architectural imitation porcelain coating described in claim 1, comprises the steps:
[0013] (1) Add tap water in the amount of the coating base material glue formula into the reaction kettle, then pass in steam to heat up to 90°C, add polyvinyl alcohol while stirring, and after the polyvinyl alcohol is completely dissolved, cool down to the glue solution at 80°C ℃;
[0014] (2) Under stirring, add hydrochloric acid in...
PUM
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com