Environment-friendly building outer wall simulated tile coating and preparation method thereof
An environmentally friendly and architectural technology, applied in the coating and other directions, can solve the problems of high cost, heavy ceramic tile, easy to fall off, etc., and achieve the effect of long service life, good shrinkage resistance and prolonging construction period.
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Examples
Embodiment Construction
[0012] (1) Extract the raw materials according to the following parts by weight ratio:
[0013] 80-100 parts by weight of water, 25-35 parts by weight of titanium dioxide, 600-800 parts by weight of colored sand, 2-4 parts by weight of dispersant, 25-35 parts by weight of cellulose ether aqueous solution with a weight concentration of 2%, pure acrylic emulsion 110-130 parts by weight, 6-10 parts by weight of ethylene glycol, 4-7 parts by weight of thickener, 6-10 parts by weight of film-forming aid, 1-2 parts by weight of defoamer, 1.5-2.5 parts by weight of preservative 1.5-2.5 parts by weight of multifunctional additives; 5040 is used for dispersant, hydroxyethyl cellulose ER30000 is used for cellulose ether, and 163M and R860 are used for pure acrylic emulsion in an optional ratio of 3:1 to 2:1. composition.
[0014] (2) Sieve the pure acrylic emulsion obtained in step (1) with a 20-mesh sieve, and then stir it with the rest of the liquid materials evenly.
[0015] (3) Mi...
PUM
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com