Method for manufacturing environment-friendly high-strength anti-deformation solid wood composite door
A solid wood composite, green and environmentally friendly technology, applied in the jointing of wooden veneers, manufacturing tools, wood processing equipment, etc., can solve the problems of not being able to find customer resources, increase the cost of raw materials, waste wood resources, etc., and achieve the purpose of saving forest resources , prevent cracking, and protect the ecological environment
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Image
Examples
Embodiment 1
[0054] A method for manufacturing a green, environment-friendly, high-strength, deformation-resistant solid wood composite door, comprising the following steps:
[0055] The first step is to soften the logs first, and then miniaturize them to make veneers;
[0056] In the second step, the veneer is divided into super-grade and first-grade panels, and second-grade and third-grade core materials, and then the selected grades of veneer are dried;
[0057] The third step is to trim the edges of the veneer boards and splice them into a whole board with a patchwork machine, then grade the whole board again, separate the face plate and core material, and then select the whole board with transverse grain from the core material as a balance The tension board and the balanced tension board are respectively placed on the center layer, the third layer below the upper surface layer, and the third layer above the lower surface layer. glue;
[0058] The fourth step is to press th...
Embodiment 2
[0062] The manufacturing method of the green, environment-friendly, high-strength and anti-deformation solid wood composite door described in this embodiment, the first step is to soften the logs, which is to cook and soften the logs. When the temperature of the logs stored outdoors is below 0°C, first Soak the logs in water at 25-35°C for 6-10 hours, and then steam the water with steam at 1.5 to 3 atmospheres; the miniaturization treatment is to make thin wood boards by cutting or peeling the logs into thin wood boards. First, put the log on the planer or rotary cutter, adjust the speed, adjust the thickness to 2mm, and cut the log into 1.8-2mm thin boards.
Embodiment 3
[0064] In the manufacturing method of the green, environment-friendly, high-strength and anti-deformation solid wood composite door described in this embodiment, the second step is to classify the veneers, select super-grade veneers and first-grade veneers as panels, and select second-grade veneers and third-grade veneers. The veneer is used as the core material, and then the selected level of veneer is dried by a hot-press drying method; the hot-press drying method uses a multi-layer hot press, and the veneer is first laid flat in the hot press After heating and pressurizing, the pressure is adjusted to 1mpa, the temperature is adjusted to be within 100°C, and the pressure is reset to zero after pressing for 30-60 seconds. Repeat several times to make the moisture content of the veneer within 6-12%.
[0065] In the manufacturing method of the green and environment-friendly high-strength anti-deformation solid wood composite door, the second step is to make the core material...
PUM
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com