Method for extracting tellurium from high-selenium content silver concentrate
A technology of silver concentrate and high selenium, which is applied in the field of tellurium extraction, can solve the problems of low tellurium recovery rate and poor raw material adaptability, and achieve the effect of increasing recovery rate and reducing impact
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Image
Examples
Embodiment
[0039] Tellurium slag is produced by smelting in a silver-splitting furnace. When the oxidation and refining progresses to the later stage, the operator takes out the alloy from the bottom of the molten pool to judge that the silver grade in the alloy is greater than 90% and starts to produce tellurium slag. The furnace temperature is controlled at 900 ° C ~ 1200 ° C, adding Stir with 10-30kg of sodium nitrate, and add 100-200kg of sodium carbonate after the reaction is complete or while adding sodium nitrate, and stir at the same time. After the stirring is completed, shake the furnace mouth to an angle of 85 degrees to the horizontal plane, insert an ordinary welded steel pipe with a diameter of Φ20mm into the furnace, and blow compressed air into the furnace to blow the slag for 2 hours. After the reaction is complete, take out the oxidation air pipe, replace the slag bag, observe the situation in the furnace and carry out the slag removal operation. The recovery rate of the...
PUM
Login to View More Abstract
Description
Claims
Application Information
Login to View More - R&D
- Intellectual Property
- Life Sciences
- Materials
- Tech Scout
- Unparalleled Data Quality
- Higher Quality Content
- 60% Fewer Hallucinations
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2025 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com