After finishing process for ready-to-wear clothes

A post-finishing and garment-making technology, which is applied in fiber treatment, dry-cleaning fiber products, textiles, and papermaking. It can solve problems such as large shrinkage, troublesome storage and ironing, and serious wrinkles, and achieves good durability and remarkable non-ironing effect. Effect

Inactive Publication Date: 2014-03-19
江苏常朔针纺纱科技有限公司
View PDF2 Cites 5 Cited by
  • Summary
  • Abstract
  • Description
  • Claims
  • Application Information

AI Technical Summary

Problems solved by technology

[0002] Natural fiber clothing, such as cotton, linen, tencel, etc., has a large shrinkage rate after washing, serious wrinkles, troublesome storage and ironing, and it is difficult to remove oil stains

Method used

the structure of the environmentally friendly knitted fabric provided by the present invention; figure 2 Flow chart of the yarn wrapping machine for environmentally friendly knitted fabrics and storage devices; image 3 Is the parameter map of the yarn covering machine
View more

Examples

Experimental program
Comparison scheme
Effect test

Embodiment 1

[0016] A finishing process for ready-made garments, comprising the steps of:

[0017] 1) Desizing: Put the white soap oil into the washing machine, heat up to 50°C, wash with water for 50 minutes, then rinse with water, adjust the pH value to 5.9 with glacial acetic acid, and wash for 25 minutes;

[0018] 2) Dehydration: water squeeze rate 55%;

[0019] 3) Drying: steam pressure 2 kg;

[0020] 4) Immersion working solution: take 20 parts by mass of fatty alcohol polyoxyethylene ether, 30 parts by mass of modified methylol dihydroxyethylene urea, 2 parts by mass of sodium laurylaminoethyl sulfate, and 40 parts by mass of bifunctional denatured N-hydroxyformic acid Amine, 3 parts by mass of coconut oil fatty acid monoethanolamide, and 25 parts by mass of magnesium chloride are mixed and stirred evenly, and the pH value is adjusted to 4.5 with glacial acetic acid with a concentration of 50%. liquid, evenly adsorbed for 40 minutes;

[0021] 5) Second drying: the moisture conten...

Embodiment 2

[0025] A finishing process for ready-made garments, comprising the steps of:

[0026] 1) Desizing: Put the white soap oil into the washing machine, heat up to 45°C, wash with water for 45 minutes, then rinse with water, adjust the pH value to 5.7 with glacial acetic acid, and wash for 20 minutes;

[0027] 2) Dehydration: water squeeze rate 50%;

[0028] 3) Drying: steam pressure 1 kg;

[0029] 4) Immersion working solution: Take 10 parts by mass of fatty alcohol polyoxyethylene ether, 25 parts by mass of modified methylol dihydroxyethylene urea, 1 part by mass of sodium lauroylaminoethyl sulfate, and 35 parts by mass of bifunctional denatured N-hydroxyformic acid Amine, 2 parts by mass of coconut oil fatty acid monoethanolamide, and 10 parts by mass of magnesium chloride are mixed and stirred evenly, and the pH value is adjusted to 4 with glacial acetic acid with a concentration of 45%, and the ready-made clothes are put into the dipping machine, and then poured into 65% of t...

Embodiment 3

[0034] A finishing process for ready-made garments, comprising the steps of:

[0035] 1) Desizing: Put the white soap oil into the washing machine, heat up to 48°C, wash with water for 47 minutes, then rinse with water, adjust the pH value to 5.8 with glacial acetic acid, and wash for 23 minutes;

[0036] 2) Dehydration: water squeeze rate 52%;

[0037] 3) Drying: steam pressure 1.2 kg;

[0038] 4) Soaking working solution: Take 16 parts by mass of fatty alcohol polyoxyethylene ether, 29 parts by mass of modified methylol dihydroxyethylene urea, 1.2 parts by mass of sodium laurylaminoethyl sulfate, and 37 parts by mass of bifunctional denatured N-carboxylic acid Amine, 2.3 parts by mass of coconut oil fatty acid monoethanolamide, and 18 parts by mass of magnesium chloride are mixed and stirred evenly, and the pH value is adjusted to 4.3 with glacial acetic acid with a concentration of 48%, and the ready-made clothes are put into the dipping machine, and then poured into the w...

the structure of the environmentally friendly knitted fabric provided by the present invention; figure 2 Flow chart of the yarn wrapping machine for environmentally friendly knitted fabrics and storage devices; image 3 Is the parameter map of the yarn covering machine
Login to view more

PUM

No PUM Login to view more

Abstract

The invention discloses an after finishing process for read-to-wear clothes. The after finishing process comprises the following steps: (1) desizing: putting a white detergent agent into a washing machine, heating to 45-50 DEG C, washing with water for 45-50 minutes, washing with clear water once again, adjusting the pH value to 5.7-5.9 with glacial acetic acid, and washing for 20-25 minutes; (2) dehydrating, wherein the squeezing rate is 50-55 percent; (3) drying, wherein steam pressure is 1-2 kilograms; (4) soaking into a working liquid; (5) performing secondary drying till the water content is 8-9 percent, and cooling in an air cooler for 15-20 minutes; (6) pressing at the temperature of 140-145 DEG C for 9-11 seconds and under the pressure of 6-7 kilograms, and baking at the temperature of 165-170 DEG C for 15-20 minutes; (7) cooling in a wet room of which the temperature is 23-25 DEG C and the humidity is 90-95 percent for 1-2 hours. The read-to-wear clothes finished with the after finishing process has the advantages of water resistance, oil resistance, stain resistance, remarkable non-ironing effect and high durability.

Description

technical field [0001] The present invention relates to the post-finishing process of finished garments. Background technique [0002] Natural fiber clothing such as cotton, linen, tencel, etc., has a large shrinkage rate after washing, serious wrinkles, troublesome storage and ironing, and it is difficult to remove oil stains. Contents of the invention [0003] The purpose of the present invention is to provide a finishing process for ready-made garments. The finished garments are waterproof, oil-proof, stain-proof, non-ironing effect is remarkable, and durability is good. [0004] In order to achieve the above object, the technical solution of the present invention is to design a kind of finishing process of ready-made clothes, comprising the steps: [0005] 1) Desizing: Put the white soap oil into the washing machine, heat up to 45-50°C, wash with water for 45-50 minutes, then rinse with water, adjust the pH value to 5.7-5.9 with glacial acetic acid, and wash for 20-25...

Claims

the structure of the environmentally friendly knitted fabric provided by the present invention; figure 2 Flow chart of the yarn wrapping machine for environmentally friendly knitted fabrics and storage devices; image 3 Is the parameter map of the yarn covering machine
Login to view more

Application Information

Patent Timeline
no application Login to view more
Patent Type & Authority Applications(China)
IPC IPC(8): D06M15/53D06M13/325D06M13/432D06M11/155D06L1/14D06M101/06
Inventor 庄家杰
Owner 江苏常朔针纺纱科技有限公司
Who we serve
  • R&D Engineer
  • R&D Manager
  • IP Professional
Why Eureka
  • Industry Leading Data Capabilities
  • Powerful AI technology
  • Patent DNA Extraction
Social media
Try Eureka
PatSnap group products