Feldspar and quartz flotation separation method
A quartz and feldspar technology, applied in the field of mineral flotation separation, can solve the problems of environmental pollution and high requirements for flotation equipment, and achieve the effect of reducing production costs, low requirements for flotation equipment and less environmental pollution.
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Examples
Embodiment 1
[0014] Embodiment 1, the method for flotation separation of feldspar and quartz is carried out according to the following steps: the first step, the feldspar and quartz raw ore are firstly ground, and in the grinding process, 100g to 800g of carbonic acid is added per ton of feldspar and quartz raw ore Sodium meter: Add sodium carbonate to feldspar and quartz raw ore, and mix the ground feldspar and quartz raw ore with water to form a slurry with a mass concentration of 10% to 50%; in the second step, add 50g to 1000gN per ton of feldspar and quartz raw ore - Acyl sarcosine sodium meter Weigh N-acyl sarcosine sodium, prepare the weighed N-acyl sarcosine sodium water into a cleaning solution with a mass concentration of 5% to 10%, and add the cleaning solution to the pulp In the flotation machine, the raw ore pulp is obtained after stirring for 5 to 40 minutes in the flotation machine; in the third step, 10g to 1000g of collector A is added to the raw ore pulp in the flotation...
Embodiment 2
[0015] Embodiment 2, the method for feldspar and quartz flotation separation is carried out according to the following steps: the first step, the feldspar and quartz raw ore are first passed through ore grinding, and 100g or 800g of carbonic acid is added per ton of feldspar and quartz raw ore in the grinding process Sodium meter: Add sodium carbonate to feldspar and quartz raw ore, and mix the ground feldspar and quartz raw ore with water to form a slurry with a mass concentration of 10% or 50%; in the second step, add 50g or 1000gN per ton of feldspar and quartz raw ore -Acyl sarcosine sodium meter Weigh N-acyl sarcosine sodium, prepare the weighed N-acyl sarcosine sodium water into a cleaning solution with a mass concentration of 5% or 10%, and add the cleaning solution to the pulp In the flotation machine, the raw ore pulp is obtained after stirring for 5 minutes or 40 minutes; in the third step, 10g or 1000g of collector A is added to the raw ore pulp in the flotation ma...
Embodiment 3
[0016] Embodiment 3, the difference with the above-described embodiment is that after preparing the slurry and before the second step, add 100g to 1000g sodium carbonate per ton of feldspar and quartz raw ore to weigh the sodium carbonate, and take the weighed carbonic acid Prepare sodium carbonate aqueous solution with a mass concentration of 1% to 20% with sodium water, add the sodium carbonate aqueous solution to the pulp, stir and mix evenly, and then add the prepared cleaning solution to it.
PUM
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com