Building external wall thermal insulating powder coating, and preparation method thereof
A thermal insulation and powder coating technology, which is applied in the field of architectural coatings, can solve the problems of poor thermal insulation and thermal insulation performance, poor coating adhesion, and no elasticity, so as to improve coating protection performance and improve coating decoration. , The effect of simple construction
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Examples
Embodiment 1
[0054] In the single-mix dry powder mortar mixer, add the following components in sequence by weight: 16 parts of white Portland cement (325 type), 1.6 parts of high alumina cement (Suihua brand special cement), 8 parts of closed hollow ceramic particles ( Guangzhou Ceramic Building Material Factory), 3 parts of nano-infrared reflective powder (Schetter, USA), 1 part of vinyl acetate-ethylene polymer (Wacker), 0.05 part of methyl hydroxyethyl cellulose ether (Bayer), 0.2 part Defoamer (Hexon), 0.1 part of water reducer, 0.15 part of water repellent (Wacker), 8 parts of kaolin (800 mesh), 7 parts of heavy calcium (400 mesh), 0.01 part of alkali-resistant glass fiber, 15 parts of river Sand (20 mesh), 25 parts of river sand (40 mesh) and 15 parts of river sand (80 mesh) were stirred and mixed evenly to obtain the thermal insulation powder coating.
Embodiment 2
[0056] In the single-mix dry powder mortar mixer, add the following components in sequence by weight: 18 parts of white Portland cement (325 type), 1.8 parts of high alumina cement (Suihua brand special cement), 10.5 parts of closed hollow ceramic particles ( Guangzhou Ceramic Building Material Factory), 5 parts of nano-infrared reflective powder (Schetter, USA), 2 parts of vinyl acetate-ethylene polymer (Wacker), 0.09 part of methyl hydroxyethyl cellulose ether (Bayer), 0.2 part Defoamer (Hexion), 0.15 parts of water reducing agent, 0.25 parts of water repellent (Wacker), 8 parts of kaolin (800 mesh), 7 parts of heavy calcium (400 mesh), 0.01 part of anti-alkali glass fiber, 12 parts of river Sand (20 mesh), 20 parts of river sand (40 mesh) and 15 parts of river sand (80 mesh) were stirred and mixed evenly to obtain the thermal insulation powder coating.
Embodiment 3
[0058] In the single-mix dry powder mortar mixer, add the following components in sequence by weight: 18 parts of white Portland cement (325 type), 1.8 parts of high alumina cement (Suihua brand special cement), 12.5 parts of closed hollow ceramic particles ( Guangzhou Ceramic Building Material Factory), 5 parts of nano-infrared reflective powder (Schetter, USA), 2 parts of vinyl acetate-ethylene polymer (Wacker), 0.09 part of methyl hydroxyethyl cellulose ether (Bayer), 0.2 part Defoamer (Hexon), 0.15 parts of water reducing agent, 0.25 parts of water repellent (Wacker), 8 parts of kaolin (800 mesh), 7 parts of heavy calcium (400 mesh), 0.01 part of alkali-resistant glass fiber, 10 parts of river Sand (20 mesh), 20 parts of river sand (40 mesh) and 15 parts of river sand (80 mesh) were stirred and mixed evenly to obtain the thermal insulation powder coating.
PUM
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com