Aqueous coating for decorating inner wall of antifouling building and preparation method of aqueous coating
A building, water-based technology, applied in antifouling/underwater coatings, coatings, paints containing biocides, etc., to achieve the effect of large brushing area, blocking stains immersion, and good construction performance
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Examples
Embodiment 1
[0016] A water-based coating for anti-fouling building interior wall decoration, which consists of the following components by weight: 15 parts of deionized water, 0.7 parts of wetting and dispersing agent, 0.2 parts of defoaming agent, 1.5 parts of propylene glycol, 18 parts of titanium dioxide, 6 parts of kaolin, 7 parts of talcum powder, 9 parts of wollastonite powder, 3.5 parts of nano-scale anti-fouling additives, 35 parts of nano-scale acrylic emulsion, 0.3 parts of bactericide, 1.5 parts of film-forming aids, pH adjustment 0.15 parts of agent, 0.4 parts of thickener.
[0017] Example 1 The kaolin is 4000 mesh, the talcum powder is 1250 mesh, and the silica lime powder is 1250 mesh.
[0018] The preparation method of the antifouling building interior wall decoration water-based coating comprises the following steps: (1) mixing deionized water, wetting and dispersing agent, defoaming agent and propylene glycol, adding titanium dioxide, kaolin, talcum powder and wollastoni...
Embodiment 2
[0020] A water-based coating for anti-fouling building interior wall decoration, which consists of the following components in parts by weight: 10 parts of deionized water, 0.5 parts of wetting and dispersing agent, 0.1 part of defoaming agent, 1 part of propylene glycol, 15 parts of titanium dioxide, 8 parts of kaolin, 5 parts of talcum powder, 8 parts of wollastonite powder, 2 parts of nano-scale anti-fouling additives, 32 parts of nano-scale acrylic emulsion, 0.2 parts of fungicide, 1 part of film-forming aid, pH adjustment 0.1 part of agent, 0.3 part of thickener.
[0021] Example 2 The kaolin is 4000 mesh, the talcum powder is 1250 mesh, and the silica lime powder is 1250 mesh. ,
[0022] The preparation method of the antifouling building interior wall decoration water-based coating comprises the following steps: (1) mixing deionized water, wetting and dispersing agent, defoaming agent and propylene glycol, adding titanium dioxide, kaolin, talcum powder and wollastonite ...
Embodiment 3
[0024] A water-based paint for anti-fouling building interior wall decoration, which consists of the following components in parts by weight: 20 parts of deionized water, 0.8 parts of wetting and dispersing agent, 0.3 parts of defoaming agent, 2 parts of propylene glycol, 20 parts of titanium dioxide, 5 parts of kaolin, 10 parts of talcum powder, 10 parts of wollastonite powder, 5 parts of nano-scale anti-fouling additives, 40 parts of nano-scale acrylic emulsion, 0.5 parts of bactericide, 2 parts of film-forming aids, pH adjustment 0.2 parts of agent, 0.5 parts of thickener.
[0025] Example 3 The kaolin is 4000 mesh, the talcum powder is 1250 mesh, and the silica lime powder is 1250 mesh.
[0026] The preparation method of the antifouling building interior wall decoration water-based coating comprises the following steps: (1) mixing deionized water, wetting and dispersing agent, defoaming agent and propylene glycol, adding titanium dioxide, kaolin, talcum powder and wollasto...
PUM
Login to View More Abstract
Description
Claims
Application Information
Login to View More - R&D
- Intellectual Property
- Life Sciences
- Materials
- Tech Scout
- Unparalleled Data Quality
- Higher Quality Content
- 60% Fewer Hallucinations
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2025 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com