Paint coating
A paint and coating technology, applied in the field of paint and coating, can solve the problems of easy peeling, many harmful components, poor viscosity, etc., and achieves the effect of satisfying the needs of the use effect, the production method is simple, and the drying is fast.
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Examples
Embodiment 1
[0015] In the embodiment of the present invention, a paint coating is extracted according to the amount of each content: 20 parts of paint powder, 5 parts of polyvinyl butyral, 5 parts of zeolite powder, 40 parts of water solvent, 10 parts of butanol and methyl ethyl ketone mixture, 4 parts of water-soluble resin, 3.5 parts of non-leafing aluminum powder slurry, 11 parts of acrylonitrile, 3 parts of methyl methacrylate, 10 parts of a mixture of rosin resin and linseed oil, and 1 part of phosphoric acid; the specific preparation method is, first, paint powder 20 parts, 5 parts of polyvinyl butyral, 5 parts of zeolite powder, 40 parts of water solvent, 10 parts of butanol and methyl ethyl ketone mixture, 4 parts of water-soluble resin, 3.5 parts of non-leafing aluminum powder slurry, 11 parts of acrylonitrile and methyl ethyl ketone Put 3 parts of methyl acrylate into the processing equipment, and the temperature is controlled at 45°C-75°C; then stir for 10-15 minutes to make it ...
Embodiment 2
[0017] A paint coating, extracted according to the amount of each content: 25 parts of paint powder, 7 parts of polyvinyl butyral, 8 parts of zeolite powder, 45 parts of water solvent, 13 parts of a mixture of butanol and methyl ethyl ketone, 5 parts of water-soluble resin, 3.7 parts of floating aluminum powder slurry, 11 parts of acrylonitrile, 4 parts of methyl methacrylate, 15 parts of a mixture of rosin resin and linseed oil, and 2 parts of phosphoric acid; the specific preparation method is, first, 25 parts of paint powder, polyvinyl alcohol 7 parts of butyral, 8 parts of zeolite powder, 45 parts of water solvent, 13 parts of butanol and methyl ethyl ketone mixture, 5 parts of water-soluble resin, 3.7 parts of non-leafing aluminum powder slurry, 11 parts of acrylonitrile and 4 parts of methyl methacrylate Put it into the processing equipment, the temperature is controlled at 45°C-75°C; then stir for 10-15 minutes to make it uniform and form a thinner paint; then, add rosin...
Embodiment 3
[0019] A kind of paint, extracted according to the amount of each content: 30 parts of paint powder, 9 parts of polyvinyl butyral, 10 parts of zeolite powder, 50 parts of water solvent, 15 parts of butanol and methyl ethyl ketone mixture, 6 parts of water-soluble resin, 3.8 parts of floating aluminum powder slurry, 12 parts of acrylonitrile, 5 parts of methyl methacrylate, 18 parts of a mixture of rosin resin and linseed oil, and 3 parts of phosphoric acid; the specific preparation method is, first, 30 parts of paint powder, polyvinyl alcohol 9 parts of butyral, 10 parts of zeolite powder, 50 parts of water solvent, 15 parts of butanol and methyl ethyl ketone mixture, 6 parts of water-soluble resin, 3.8 parts of non-leafing aluminum powder slurry, 12 parts of acrylonitrile and 5 parts of methyl methacrylate Put it into the processing equipment, control the temperature at 45°C-75°C, and then stir it for 10-15 minutes to make it uniform and form a thinner paint; then, add rosin r...
PUM
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com