A kind of M85 methanol gasoline and preparation method thereof

A methanol gasoline and gasoline technology, applied in the petroleum industry, liquid carbon-containing fuel, fuel, etc., can solve the problems of limited promotion and application of methanol gasoline, narrowing the application range of methanol gasoline, and difficult storage of methanol gasoline, and achieves the improvement of water contact Delamination limit value, reduced storage difficulty, reduced rubber swelling effect

CN104804778BActive Publication Date: 2016-08-24贵州大洋能源有限责任公司
3 Cites 0 Cited by

Patent Information

Authority / Receiving Office
CN · China
Patent Type
Patents(China)
Current Assignee / Owner
Publication Date
2016-08-24
Patent Text Reader

Abstract

The invention relates to the technical field of methanol gasoline, in particular to an M85 methanol gasoline and a preparation method thereof. According to the preparation method, methanol, gasoline, sodium methoxide, pine oil, waste oil, glycerin, acetone and polyoxyethylene ether are mixed according to a proportion; the pine oil and the waste oil are separately treated through the combination of preparation process steps; the treated pine oil and waste oil are added for mixing; ultrasonic mixing treatment is performed during treatment processes, so that all raw materials are dispersed more uniformly, mutual concurrent effects among the methanol, gasoline, waste oil and other raw materials are further achieved, and then the quality of the methanol gasoline is improved. Particularly, the phenomenon that the methanol gasoline is easy to be subjected to stratification when the water content reaches 3% is avoided. Therefore, the water resistance of the methanol gasoline is improved, the guarantee period of the methanol gasoline is prolonged, and the storage difficulty of the methanol gasoline is lowered.
Need to check novelty before this filing date? Find Prior Art

Description

technical field

[0001] The invention relates to the technical field of methanol gasoline, in particular to M85 methanol gasoline and a preparation method thereof. Background technique

[0002] With the increase of the global population and the continuous improvement of people's living standards, the demand for energy is becoming stronger and stronger. Especially with the rapid development of petrochemical industry in the mid-20th century, the pace of energy industry development has been accelerated. Petroleum consumption is increasing year by year, and the environmental pollution caused by the burning of petroleum products is becoming more and more serious. Using petroleum products as fuel, the carbon, nitrogen, sulfur oxides, and hydrocarbons contained in the tail gas of automobiles are harmful to the environment. caused great harm. At the same time, this has also made traditional oil and natural gas resources increasingly scarce. According to surveys, the world's proven ...

Examples

Embodiment 1

[0029] A kind of M85 methanol gasoline, the raw material composition by weight percentage is methanol 85%, gasoline 5%, sodium methoxide 2%, pine oil 0.9%, waste oil 5.1%, glycerin 1%, acetone 0.3%, polyoxyethylene ether 0.7% %.

[0030] Described gasoline is 93# gasoline.

[0031] Its preparation method comprises the following steps:

[0032] (1) Mix gutter oil and pine oil according to the ratio, put them in an ultrasonic processor, use ultrasonic frequency of 30KHz to treat for 10min, and adjust the temperature during the processing to maintain at 70°C, after the ultrasonic treatment is completed , and then carry out the cooling treatment, the cooling treatment is to cool the oil at 70°C to a temperature of 1°C in 10 hours, and then place it in a vacuum filter for suction filtration to obtain grease;

[0033] (2) Mix the oil obtained in step 1) with methanol and sodium methoxide in an environment of 30°C, and stir at a stirring speed of 120r / min for 30min, then add glycer...

Embodiment 2

[0040] A kind of M85 methanol gasoline, the raw material components are 85% of methanol, 3% of gasoline, 1.2% of sodium methoxide, 0.9% of pine oil, 7% of waste oil, 2% of glycerin, 0.5% of acetone, and 0.4% of polyoxyethylene ether. %.

[0041] Described gasoline is 93# gasoline.

[0042] Its preparation method comprises the following steps:

[0043] (1) Mix gutter oil and pine oil according to the ratio, put them in an ultrasonic processor, use ultrasonic frequency of 60KHz to treat for 20min, and adjust the temperature during the processing to maintain at 90°C, after the ultrasonic treatment is completed , and then carry out cooling and cooling treatment. The cooling and cooling treatment is to cool the oil at 90°C to a temperature of 5°C in 12 hours, and then place it in a vacuum filter for suction filtration to obtain grease;

[0044] (2) Mix the oil obtained in step 1) with methanol and sodium methoxide in an environment of 50°C, and stir at a stirring speed of 170r / mi...

Embodiment 3

[0051] A kind of M85 methanol gasoline, the raw material components are 85% of methanol, 4% of gasoline, 1.5% of sodium methoxide, 0.8% of pine oil, 7% of waste oil, 1% of glycerin, 0.3% of acetone, and 0.4% of polyoxyethylene ether. %.

[0052] Described gasoline is 93# gasoline.

[0053] Its preparation method comprises the following steps:

[0054] (1) Mix gutter oil and pine oil according to the ratio, put them in an ultrasonic processor, use ultrasonic frequency of 40KHz to treat for 15min, and adjust the temperature during the processing to maintain at 80°C, after the ultrasonic treatment is completed , and then carry out the cooling treatment, the cooling treatment is to cool the oil at 80°C to a temperature of 3°C in 11 hours, and then place it in a vacuum filter for suction filtration to obtain grease;

[0055] (2) Mix the oil obtained in step 1) with methanol and sodium methoxide in an environment of 40°C, and use a stirring speed of 150r / min to stir for 40min, and...