A production method and technology of shampoo, which is applied in hair care, pharmaceutical formulations, cosmetic preparations, etc., can solve the problems of dry hair, allergies, roughness and not suppleness, etc., to reduce the generation of dandruff, reduce the absorption of dust, reduce the The effect of the frequency of shampooing
Patent Information
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Publication Date
- 2015-10-21
- Estimated Expiration
- Not applicable · inactive patent
Smart Images
Figure 1 Figure 2
Abstract
Description
technical field
[0001] The invention relates to a shampoo and a preparation method thereof. Background technique
[0002] Nowadays, people are widely using chemical shampoos to shampoo their hair. Due to the high content of chemical components, there are many substances with acid radicals. People will wash their hair every day as a temporary improvement, but washing their hair every day will cause a vicious cycle of this phenomenon and make the hair more dry; as well as problems such as scalp seborrheic inflammation and allergies, it will also cause the discharge of sewage after shampooing Water pollution is formed, and the harm of this pollution cannot be obvious in a short time. Contents of the invention
[0003] In view of the above problems, the object of the present invention is to provide a shampoo and a preparation method thereof.
[0004] In order to achieve the above object, a shampoo according to the present invention comprises: 0.1-0.3 parts of cationic guar g...
Examples
Embodiment 1
[0028] The preparation method of a shampoo described in this embodiment includes adding the ionic calcium water-soluble preparation in at least one step in the process of making the shampoo.
[0029] The specific steps are:
[0030] 1) Add 0.1 part of cationic guar gum to 100 parts of demineralized water for stirring and dissolving;
[0031] 2) Heat the guar gum solution in step 1) to 60°C, and add 0.2 parts of ammonium lauryl alcohol ether sulfate, 0.15 parts of natural fatty alcohol ether ammonium sulfate, 0.1 part of behenyltrimethyl Ammonium chloride, 1 part of surfactant, 2 parts of anti-dandruff agent, 0.5 part of pearl paste, and 2 parts of silicone emulsion were stirred for 2 hours and then cooled to 30°C;
[0032] 3) Add 5 parts of nonionic surfactant, 2 parts of protein polymer, 10 parts of softener, 15 parts of essence and 100 parts of distilled water into a high-speed homogeneous vacuum emulsification tank, heat it to 70°C and let it stand for 30 minutes to dissol...
Embodiment 2
[0039]The preparation method of a shampoo described in this embodiment includes adding the ionic calcium water-soluble preparation in at least one step in the process of making the shampoo.
[0040] The specific steps are:
[0041] 1) Add 0.3 parts of cationic guar gum to 100 parts of demineralized water for stirring and dissolving;
[0042] 2) Heat the guar gum solution in step 1) to 70°C, and add 0.6 parts of ammonium lauryl alcohol ether sulfate, 0.45 parts of natural fatty alcohol ether ammonium sulfate, 0.3 parts of behenyltrimethyl Ammonium chloride, 3 parts of surfactant, 6 parts of anti-dandruff agent, 1.5 parts of pearl paste, and 6 parts of silicone emulsion were stirred for 3 hours and then cooled to 30-40°C;
[0043] 3) Add 8 parts of nonionic surfactant, 5 parts of protein polymer, 12 parts of softener, 20 parts of essence and 100 parts of distilled water into a high-speed homogeneous vacuum emulsification tank, heat it to 80°C and let it stand for 45 minutes to ...
Embodiment 3
[0050] The preparation method of a shampoo described in this embodiment includes adding the ionic calcium water-soluble preparation in at least one step in the process of making the shampoo.
[0051] The specific steps are:
[0052] 1) Add 0.2 parts of cationic guar gum to 100 parts of demineralized water for stirring and dissolving;
[0053] 2) Heat the guar gum solution in step 1) to 65°C, and add 0.4 parts of ammonium lauryl alcohol ether sulfate, 0.3 parts of natural fatty alcohol ether ammonium sulfate, 0.2 parts of behenyltrimethyl Ammonium chloride, 2 parts of surfactant, 4 parts of anti-dandruff agent, 0.8 part of pearl paste, 4 parts of silicone emulsion were stirred for 2.5 hours and then cooled to 35°C;
[0054] 3) Add 7 parts of nonionic surfactant, 4 parts of protein polymer, 11 parts of softener, 18 parts of essence and 100 parts of distilled water into a high-speed homogeneous vacuum emulsification tank, heat it to 75°C and let it stand for 40 minutes to dissol...