Chlor-alkali wastewater treating agent and preparation method thereof
A wastewater treatment agent, chlor-alkali technology, applied in water/sewage treatment, water/sludge/sewage treatment, chemical instruments and methods, etc., can solve the problems of organic matter degradation in water, high COD in water, increase in water salinity, etc. To achieve the effect of low cost, good treatment effect and easy operation
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Examples
Embodiment 1
[0029] In the embodiment of the present invention, the chlor-alkali wastewater treatment agent is composed of the following raw materials in parts by weight:
[0030] 30 parts of sodium silicate
[0031] 60 parts limestone
[0032] 20 parts of triethoxysilyl propyl glyceryl ether
[0033] 15 parts of citric acid.
[0034] In the preparation method of the chlor-alkali wastewater treatment agent, citric acid is added with water to prepare a citric acid aqueous solution with a concentration of 2 mol / l. Put the sodium silicate and citric acid aqueous solution into the reaction kettle and heat and stir for 1 hour at a heating temperature of 50°C; add triethoxy silylpropyl glycerol ether into the reaction kettle and heat and stir for 5 hours under a nitrogen atmosphere at a heating temperature of 70 ℃. Then the temperature is lowered to 30°C, limestone is added, and stirred for 5 hours to obtain the chlor-alkali wastewater treatment agent.
Embodiment 2
[0036] In the embodiment of the present invention, the chlor-alkali wastewater treatment agent is composed of the following raw materials in parts by weight:
[0037] 50 parts of sodium silicate
[0038] 70 parts limestone
[0039] 40 parts of triethoxysilyl propyl glyceryl ether
[0040] 40 parts of citric acid.
[0041] In the preparation method of the chlor-alkali wastewater treatment agent, citric acid is added with water to prepare an aqueous solution of citric acid with a concentration of 5 mol / l. Put the sodium silicate and citric acid aqueous solution into the reaction kettle and heat and stir for 15 hours at a heating temperature of 100°C; add triethoxysilyl glycerol ether into the reaction kettle and heat and stir for 15 hours under a nitrogen atmosphere at a heating temperature of 80 ℃. Then the temperature is lowered to 40°C, limestone is added, and the mixture is stirred for 12 hours to obtain the chlor-alkali wastewater treatment agent.
Embodiment 3
[0043] In the embodiment of the present invention, the chlor-alkali wastewater treatment agent is composed of the following raw materials in parts by weight:
[0044] 35 parts of sodium silicate
[0045] 62 parts limestone
[0046] 25 parts of triethoxy silyl propyl glyceryl ether
[0047] 25 parts of citric acid.
[0048] In the preparation method of the chlor-alkali wastewater treatment agent, citric acid is added with water to prepare an aqueous solution of citric acid with a concentration of 3 mol / l. Put the sodium silicate and citric acid aqueous solution into the reaction kettle and heat and stir for 5 hours at a heating temperature of 60°C; add triethoxysilyl glycerol ether into the reaction kettle and heat and stir for 8 hours under a nitrogen atmosphere at a heating temperature of 72 ℃. Then the temperature is lowered to 32°C, limestone is added, and stirred for 7 hours to obtain the chlor-alkali wastewater treatment agent.
PUM
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com