EVA (ethylene vinyl acetate) environment-friendly jigsaw puzzle
A toy and environmental protection technology, applied in sports accessories, indoor games, etc., can solve the problems of easy burning, poor water and dirt resistance, easy deformation, etc., and achieve good wear resistance and durability, good flame retardancy, and soft texture Effect
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Examples
Embodiment 1
[0021] In this embodiment, the EVA composition material contains the following components in terms of weight percentage: 10.0wt% low-density polyethylene, 5.5wt% magnesium oxide, 3.0wt% zinc oxide, 1.0wt% three Allyl isocyanurate, 1.2 wt% polybutenyl succinate, 0.8 wt% vinyltriacetoxysilane, 2.0 wt% microcrystalline paraffin, 1.2 wt% azodicarbonamide , 0.8wt% iron carboxylate, 0.50wt% dicumyl peroxide, 0.15wt% antioxidant B225, and the balance of ethylene-vinyl acetate copolymer. The preparation method of the EVA composition material comprises the following steps: (1) Mixing: mixing low-density polyethylene, magnesium oxide, zinc oxide, triallyl isocyanurate, polybutenyl succinic acid according to the component ratio Ester, vinyltriacetoxysilane, microcrystalline paraffin, iron carboxylate, antioxidant B225, and ethylene-vinyl acetate copolymer are mixed uniformly in a mixer to obtain a mixture; (2) banburying: the step ( 1) Pour the obtained mixture into the banbury mixer fo...
Embodiment 2
[0023] In this embodiment, the EVA composition material contains the following components in terms of weight percentage: 12.0wt% of low-density polyethylene, 5.0wt% of magnesium oxide, 3.5wt% of zinc oxide, 0.8wt% of three Allyl isocyanurate, 1.2 wt% polybutenyl succinate, 0.8 wt% vinyltriacetoxysilane, 2.0 wt% zinc stearate, 1.2 wt% azodimethoxane Amide, 0.8wt% iron carboxylate, 0.50wt% dicumyl peroxide, 0.15wt% antioxidant B225, and the balance of ethylene-vinyl acetate copolymer. The preparation method of the EVA composition material comprises the following steps: (1) Mixing: mixing low-density polyethylene, magnesium oxide, zinc oxide, triallyl isocyanurate, polybutenyl succinic acid according to the component ratio Ester, vinyltriacetoxysilane, zinc stearate, iron carboxylate, antioxidant B225, and ethylene-vinyl acetate copolymer are mixed uniformly in a mixer to obtain a mixture; (2) banburying: the step (1) Pour the obtained mixture into a banbury mixer for 6 minutes ...
Embodiment 3
[0025]In this embodiment, the EVA composition material contains the following components in terms of weight percentage: 12.0wt% of low-density polyethylene, 5.0wt% of magnesium oxide, 3.5wt% of zinc oxide, 1.0wt% of three Allyl isocyanurate, 1.2wt% polybutenyl succinate, 0.8wt% vinyltriacetoxysilane, 2.0wt% ethylenebisstearamide, 1.2wt% Nitrogen dicarboxamide, 0.8wt% iron carboxylate, 0.50wt% dicumyl peroxide, 0.15wt% antioxidant B225, and the balance of ethylene-vinyl acetate copolymer. The preparation method of the EVA composition material comprises the following steps: (1) Mixing: mixing low-density polyethylene, magnesium oxide, zinc oxide, triallyl isocyanurate, polybutenyl succinic acid according to the component ratio Ester, vinyltriacetoxysilane, ethylenebisstearamide, iron carboxylate, antioxidant B225, and ethylene-vinyl acetate copolymer are mixed uniformly in a mixer to obtain a mixture; (2) internal mixing : Pour the mixture obtained in step (1) into a banbury mi...