An automobile weather strip and anti-aging technology, applied in the field of automobile weather strip, can solve the problem that the weather strip can no longer meet the modern industrial requirements, etc., and achieve the effects of long service life, reduced pollution and reasonable formula ratio.
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Examples
Embodiment 1
[0013] A compression-resistant and anti-aging automobile sealing strip is characterized in that the components of the raw materials are composed as follows in parts by weight:
[0014] 20 parts of EPDM rubber, 25 parts of nitrile rubber, 3 parts of tert-butyl perbenzoate, 2 parts of semi-reinforcing carbon black N6602, 2 parts of silicon dioxide, 2 parts of pentaerythritol tetrastearate, 1 part of paraffin oil , anti-aging agent DTPD and anti-aging agent MB according to the weight ratio of 2:3 composition of anti-aging agent 2 parts, silane coupling agent KH5503 parts, vulcanizing agent 1.2 parts, stearic acid 3 parts, zinc borate 4 parts, attapulgite, mica powder 8 parts of fillers composed of quartz powder according to the weight ratio of 2:2:3, and 0.4 parts of vulcanizing agent composed of vulcanizing agent DCBP and vulcanizing agent DCP according to the weight ratio of 2:1.
Embodiment 2
[0016] A compression-resistant and anti-aging automobile sealing strip is characterized in that the components of the raw materials are composed as follows in parts by weight:
[0017] 30 parts of EPDM rubber, 28 parts of nitrile rubber, 5 parts of tert-butyl perbenzoate, 4 parts of semi-reinforcing carbon black N6604, 4 parts of silicon dioxide, 5 parts of pentaerythritol tetrastearate, 3 parts of paraffin oil , anti-aging agent DTPD and anti-aging agent MB according to the weight ratio of 2:3, 3 parts of anti-aging agent, 5 parts of silane coupling agent KH5505, 1.8 parts of vulcanizing agent, 4 parts of stearic acid, 6 parts of zinc borate, attapulgite, mica powder 10 parts of fillers composed of quartz powder according to the weight ratio of 2:2:3, and 0.6 parts of vulcanizing agent composed of vulcanizing agent DCBP and vulcanizing agent DCP according to the weight ratio of 2:1.
Embodiment 3
[0019] A compression-resistant and anti-aging automobile sealing strip is characterized in that the components of the raw materials are composed as follows in parts by weight:
[0020] 25 parts of EPDM rubber, 26 parts of nitrile rubber, 4 parts of tert-butyl perbenzoate, 3 parts of semi-reinforcing carbon black N6603, 3 parts of silicon dioxide, 4 parts of pentaerythritol tetrastearate, 2 parts of paraffin oil , anti-aging agent DTPD and anti-aging agent MB according to the weight ratio of 2:3, 2.5 parts of anti-aging agent, 4 parts of silane coupling agent KH5504, 1.6 parts of vulcanizing agent, 3.5 parts of stearic acid, 5 parts of zinc borate, attapulgite, mica powder 9 parts of fillers composed of quartz powder in a weight ratio of 2:2:3, and 0.5 parts of a vulcanizing agent composed of a vulcanizing agent DCBP and a vulcanizing agent DCP in a weight ratio of 2:1.
PUM
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com