Coal-saving combustion improver and preparation method thereof
A combustion aid and mixture technology, applied in the field of coal-saving combustion aid and its preparation, can solve the problems of excessive discharge of sulfides and harmful gases, incomplete combustion of combustible substances, and insufficient utilization of thermal efficiency, etc., to achieve energy saving The effect of environmental protection is obvious, the combustion is thorough, and the effect of easy operation
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Examples
preparation example Construction
[0022] A preparation method of a coal-saving combustion-supporting agent, comprising the following steps:
[0023] 1) Weighing: Weigh 2-4 parts by weight of cerium nitrate, 20 parts by weight of sodium carbonate, 7-9 parts by weight of potassium dichromate, and 40 parts by weight of diatomaceous earth;
[0024] 2) The above-mentioned components are ball milled and sieved respectively, and the particle diameters are all 10 microns;
[0025] 3) adding sieved sodium carbonate and 20 parts by weight of water to the sieved cerium nitrate, and mixing to obtain the first mixture;
[0026] 4) Add sieved diatomaceous earth and 30 parts by weight of water to the sieved potassium dichromate, and mix to obtain the second mixture;
[0027] 5) Mix the first mixture prepared in step 3) and the second mixture prepared in step 4) evenly.
[0028] The parts by weight described above correspond to the kilograms in the examples.
Embodiment 1
[0030] A preparation method of a coal-saving combustion-supporting agent, comprising the following steps:
[0031] 1) Weighing: Weigh 3 kg of cerium nitrate, 20 kg of sodium carbonate, 8 kg of potassium dichromate, and 40 kg of diatomaceous earth;
[0032] 2) The above-mentioned components are ball milled and sieved respectively, and the particle diameters are all 10 microns;
[0033] 3) Add sieved sodium carbonate and 20 kg of water to the sieved cerium nitrate, and mix to obtain the first mixture;
[0034] 4) Add sieved diatomaceous earth and 30 kg of water to the sieved potassium dichromate, and mix to obtain the second mixture;
[0035] 5) Mix the first mixture prepared in step 3) and the second mixture prepared in step 4) evenly.
Embodiment 2
[0037] A preparation method of a coal-saving combustion-supporting agent, comprising the following steps:
[0038] 1) Weighing materials: Weigh 2 kilograms of cerium nitrate, 20 kilograms of sodium carbonate, 7 kilograms of potassium dichromate, and 40 kilograms of diatomaceous earth respectively;
[0039] 2) The above-mentioned components are ball milled and sieved respectively, and the particle diameters are all 10 microns;
[0040] 3) Add sieved sodium carbonate and 20 kg of water to the sieved cerium nitrate, and mix to obtain the first mixture;
[0041] 4) Add sieved diatomaceous earth and 30 kg of water to the sieved potassium dichromate, and mix to obtain the second mixture;
[0042] 5) Mix the first mixture prepared in step 3) and the second mixture prepared in step 4) evenly.
PUM
Login to View More Abstract
Description
Claims
Application Information
Login to View More