Durable interior wall paint and preparation method thereof

An interior wall paint, durable technology, applied in latex paint, coating and other directions, can solve the problems of human respiratory tract injury and high free formaldehyde content

Inactive Publication Date: 2016-04-20
辛范范
View PDF5 Cites 1 Cited by
  • Summary
  • Abstract
  • Description
  • Claims
  • Application Information

AI Technical Summary

Problems solved by technology

However, the existing decorative coatings have high content of free monomers, free formaldehyde, and APEO. After decoration, coughs, sore throats, and unbearable pungent odors often appear, causing serious damage to the human respiratory tract.

Method used

the structure of the environmentally friendly knitted fabric provided by the present invention; figure 2 Flow chart of the yarn wrapping machine for environmentally friendly knitted fabrics and storage devices; image 3 Is the parameter map of the yarn covering machine
View more

Image

Smart Image Click on the blue labels to locate them in the text.
Viewing Examples
Smart Image
  • Durable interior wall paint and preparation method thereof

Examples

Experimental program
Comparison scheme
Effect test

Embodiment 1

[0014] The present invention is a durable interior wall paint, which is made of the following parts by weight of raw materials: 1.5 parts of nano titanium oxide, 5 parts of titanium dioxide, 20 parts of white latex, and 6 parts of DL-1,4-dithiothreitol , 15 parts of deionized water, 2.5 parts of lauric aldehyde, 2.5 parts of sec-octylphenol polyoxyethylene ether, 2.5 parts of methyl methacrylate and 3.5 parts of 2-aminoethyl diphenylboronic acid.

[0015] A method for preparing durable interior wall paint includes the following steps:

[0016] 1) Put the nano-titanium oxide, titanium dioxide and white latex into the high-speed disperser according to the formula and stir at high speed for 15 minutes, then switch to low speed stirring for 5 minutes, and vacuum exhaust while stirring;

[0017] 2) Stir uniformly and disperse at high speed until the fineness is below 15 microns;

[0018] 3) After reducing the stirring speed, add DL-1,4-dithiothreitol, deionized water, lauric aldehyde and s...

Embodiment 2

[0022] The present invention is a durable interior wall paint made of the following parts by weight of raw materials: 3.7 parts of nano titanium oxide, 10 parts of titanium dioxide, 30 parts of white latex, and 10 parts of DL-1,4-dithiothreitol , 120 parts of deionized water, 6.3 parts of lauric aldehyde, 3.6 parts of sec-octylphenol polyoxyethylene ether, 3.7 parts of methyl methacrylate, and 4.2 parts of diphenylboronic acid-2-aminoethyl ester.

[0023] A method for preparing durable interior wall paint includes the following steps:

[0024] 1) Put the nano-titanium oxide, titanium dioxide and white latex into the high-speed disperser according to the formula, and stir at high speed for 20 minutes, then switch to low speed stirring for 10 minutes, and vacuum exhaust while stirring;

[0025] 2) Stir uniformly and disperse at high speed until the fineness is below 15 microns;

[0026] 3) After reducing the stirring speed, add DL-1,4-dithiothreitol, deionized water, lauric aldehyde and...

Embodiment 3

[0030] The present invention is a durable interior wall paint made of the following parts by weight of raw materials: 3.1 parts of nano titanium oxide, 7 parts of titanium dioxide, 23 parts of white latex, and 8.5 parts of DL-1,4-dithiothreitol , 17.5 parts of deionized water, 4.2 parts of lauric aldehyde, 3 parts of sec-octylphenol polyoxyethylene ether, 2.9 parts of methyl methacrylate, and 3.9 parts of 2-aminoethyl diphenylboronic acid.

[0031] A method for preparing durable interior wall paint includes the following steps:

[0032] 1) Put the nano-titanium oxide, titanium dioxide and white latex into the high-speed disperser according to the formula and stir at high speed for 18 minutes, then switch to low speed stirring for 8 minutes, and vacuum exhaust while stirring;

[0033] 2) Stir uniformly and disperse at high speed until the fineness is below 15 microns;

[0034] 3) After reducing the stirring speed, add DL-1,4-dithiothreitol, deionized water, lauric aldehyde and sec-octy...

the structure of the environmentally friendly knitted fabric provided by the present invention; figure 2 Flow chart of the yarn wrapping machine for environmentally friendly knitted fabrics and storage devices; image 3 Is the parameter map of the yarn covering machine
Login to View More

PUM

No PUM Login to View More

Abstract

The invention discloses durable interior wall paint. The durable interior wall paint is prepared from the following raw materials in parts by weight: 1.5-3.7 parts of nano-titania, 5-10 parts of titanium dioxide, 20-30 parts of a white emulsion, 6-10 parts of DL-1,4-dithiothreitol, 15-20 parts of deionized water, 2.5-6.3 parts of lauryl aldehyde, 2.5-3.6 parts of sec-octyl phenol polyoxyethylene ether, 2.5-3.7 parts of methyl methacrylate and 3.5-4.2 parts of diphenylboric acid-2-amino ethyl ester. Compared with emulsion paint in the prior art, the durable interior wall paint has the advantages that in the formula design, the emulsion with low VOC and odor is selected, and lauryl aldehyde extracted from plant oil is mainly taken as a film forming agent, so that the organic volatile matter which is harmful to the human body and generated by conventional film forming agents is avoided, and the durable interior wall paint is indeed healthy and environmentally friendly and is harmless to the human body. The durable interior wall paint is applicable to the decoration of public places such as hospitals, schools, office buildings, malls, hotels and the like and is particularly applicable to the decoration of sites where people and equipment cannot be evacuated.

Description

Technical field [0001] The invention relates to a durable interior wall paint and a preparation method thereof, and belongs to the field of architectural coatings. Background technique [0002] With the rapid development of the coating industry, paint home decoration has become more and more common. However, the existing decorative coatings have high free monomer and free formaldehyde content, and contain APEO. After decoration, they often have coughing, sore throat, and unbearable irritating odors, causing serious harm to the human respiratory tract. Summary of the invention [0003] In view of the shortcomings of the prior art, the technical problem to be solved by the present invention is to provide a durable interior wall paint and a preparation method thereof, which are environmentally friendly, low in odor, low in production cost, convenient in construction, and strong in adhesion. [0004] In order to solve the above technical problems, the technical solution adopted by the ...

Claims

the structure of the environmentally friendly knitted fabric provided by the present invention; figure 2 Flow chart of the yarn wrapping machine for environmentally friendly knitted fabrics and storage devices; image 3 Is the parameter map of the yarn covering machine
Login to View More

Application Information

Patent Timeline
no application Login to View More
Patent Type & Authority Applications(China)
IPC IPC(8): C09D4/06C09D4/02C09D7/12C09D5/02
CPCC09D4/06C09D5/024C09D7/61C09D7/63C08F263/04
Inventor 辛范范
Owner 辛范范