Embodiment 1
[0022] An electrical cable, comprising a core material, the core material is an iron-based alloy wire material, the core material is covered with an anti-corrosion layer, the anti-corrosion layer is covered with a light-weight braided mesh, and the light-weight braided mesh is covered with an insulating layer.
[0023] The content of each element component of the iron-based alloy wire rod is: C0.03﹪Al0.8﹪, Mg0.7﹪, Sn0.5﹪, Zn0.4﹪, Cr0.2﹪, V0.2﹪, B0.06﹪, Sr0.04﹪, Y0.02﹪, La0.01﹪, Bi0.01﹪, the balance is Fe,
[0024] The anti-corrosion layer is weighed and includes: 200 parts of chlorosulfonated polyethylene rubber, 70 parts of polycarbonate, 30 parts of orthobutyl silicate, 10 parts of neopentyl glycol, 15 parts of trioctyl trimellitate, and 100 parts of kaolin , 30 parts of barite powder and 2 parts of dibutyl maleate are mixed and solidified.
[0025] The lightweight woven net is formed by interlacing and weaving a plurality of yarns, and the yarns are blended into yarns by 3...
Embodiment 2
[0028] An electrical cable, comprising a core material, the core material is an iron-based alloy wire material, the core material is covered with an anti-corrosion layer, the anti-corrosion layer is covered with a light-weight braided mesh, and the light-weight braided mesh is covered with an insulating layer.
[0029] The content of each element component of the iron-based alloy wire rod is: C0.04﹪Al0.9﹪, Mg0.8﹪, Sn0.6﹪, Zn0.5﹪, Cr0.3﹪, V0.3﹪, B0.07﹪, Sr0.05﹪, Y0.03﹪, La0.02﹪, Bi0.02﹪, the balance is Fe,
[0030] The anti-corrosion layer is weighed and includes: 250 parts of chlorosulfonated polyethylene rubber, 80 parts of polycarbonate, 40 parts of orthobutyl silicate, 10 parts of neopentyl glycol, 15 parts of trioctyl trimellitate, and 100 parts of kaolin , 30 parts of barite powder and 2 parts of dibutyl maleate are mixed and solidified.
[0031] The lightweight woven net is formed by interlacing and weaving a plurality of yarns, and the yarns are blended into yarns by 3...
Embodiment 3
[0034] An electrical cable, comprising a core material, the core material is an iron-based alloy wire material, the core material is covered with an anti-corrosion layer, the anti-corrosion layer is covered with a light-weight braided mesh, and the light-weight braided mesh is covered with an insulating layer.
[0035] The content of each element component of the iron-based alloy wire rod is: C0.035﹪Al0.85﹪, Mg0.75﹪, Sn0.55﹪, Zn0.45﹪, Cr0.25﹪, V0.25﹪, B0.065﹪, Sr0.045﹪, Y0.025﹪, La0.015﹪, Bi0.015﹪, the balance is Fe,
[0036] The anti-corrosion layer is weighed and includes: 230 parts of chlorosulfonated polyethylene rubber, 75 parts of polycarbonate, 35 parts of orthobutyl silicate, 10 parts of neopentyl glycol, 15 parts of trioctyl trimellitate, and 100 parts of kaolin , 30 parts of barite powder and 2 parts of dibutyl maleate are mixed and solidified.