[0017] Take fresh twigs, rinse the surface with water, and then dry them naturally. When the water content is lower than 15%, use a straw grinder to crush the branches into 1cm pieces, and put the obtained pieces into pieces. Put it into an extruder and extrude it into a block, then put it into a carbonization furnace, and carbonize it at a temperature of 240 ° C for 50 minutes; after the above carbonization is completed, take it out and put it into a pulverizer for crushing Standard sieve to obtain 60-mesh carbonized cloverleaf branches particles, then put the particles into a container, add a hydrochloric acid solution with a mass fraction of 15% to soak the particles, let it stand for 30 minutes in an environment with a frequency of 20MHz, and then filter and dry , to obtain modified carbonized Cedarwood branch particles; according to mass percentage, get 45 parts of modified carbonized Cedarwood branch particles, 15 parts of deer vine root, 15 parts of bean root, 20 parts o...
example 2
[0019] Take fresh twigs, rinse the surface with water, and then dry them naturally. When the water content is lower than 15%, use a straw grinder to crush the branches into 3cm pieces, and put the obtained pieces Put it into an extruder and extrude it into a block, then put it into a carbonization furnace, and carbonize it at a temperature of 260 ° C for 70 minutes; after the above carbonization is completed, take it out and put it into a pulverizer for crushing Standard sieve to obtain 90-mesh carbonized Chinese fir branch particles, then put the particles into a container, add a hydrochloric acid solution with a mass fraction of 15% to soak the particles, let stand for 40 minutes in an environment with a frequency of 30MHz, and then filter and dry , to obtain modified carbonized Cedarwood branch particles; by mass percentage, get 50 parts of modified carbonized Cedarwood branch particles, 10 parts of deer vine root, 15 parts of bean root, 15 parts of peacock grass and 10 part...
example 3
[0021] Take fresh twigs, rinse the surface with water, and then dry them naturally. When the water content is lower than 15%, use a straw crusher to crush the branches into 2cm pieces, and put the obtained pieces Put it into an extruder and extrude it into a block, then put it into a carbonization furnace, and carbonize it at a temperature of 250°C for 60 minutes; Standard sieve to obtain 70-mesh carbonized Chinese fir branch particles, then put the particles into a container, add a hydrochloric acid solution with a mass fraction of 15% to soak the particles, let stand for 35 minutes in an environment with a frequency of 25 MHz, and then filter and dry , to obtain modified carbonized Cedarwood branch particles; according to mass percentage, get 47 parts of modified carbonized Cedarwood branch particles, 15 parts of deer vine root, 17 parts of bean root, 16 parts of peacock grass and 5 parts of distilled water , put it in a blender and stir evenly, then seal it with plastic wra...
PUM
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com