Preparation method of continuous phenolic-foam-filled honeycomb material with fixed height and thickness
A phenolic foam and honeycomb-filled technology, which is applied to the device, coating, pre-treatment surface, etc. for coating liquid on the surface, which can solve the problem of limited application, waterproof, moisture-proof, fireproof, poor thermal insulation of honeycomb materials. and other problems, to achieve the effect of a wide range of applications, excellent thermal conductivity and fire resistance, and good thermal insulation performance.
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Examples
Embodiment 1
[0021] A preparation method for continuous height-fixed thickness phenolic foam filled honeycomb material, specifically comprising the following steps: 100 parts by weight of high-performance phenolic resin, 10 parts by weight of foaming agent, 10 parts by weight of additives and 20 parts by weight of curing Agents are mixed to prepare phenolic resin glue. The above-mentioned high-performance phenolic resin has a viscosity of 1500 cps, a gel time greater than 3 minutes, and a foaming ratio of 20 times. The foaming agent is n-pentane, the additive is silicone oil, and the curing agent is phosphoric acid.
[0022] Put the prepared high-performance phenolic resin glue into the gluing device, place the honeycomb material on the operating table, turn on the gluing device, the resin glue flows out from the mouth of the gluing device evenly, and passes through the height-fixed scraper on the device. Coat the resin evenly on the surface of the honeycomb, and then send the honeycomb in...
Embodiment 2
[0024] A preparation method for continuous height-fixed thickness phenolic foam filled honeycomb material, specifically comprising the following steps: 100 parts by weight of high-performance phenolic resin, 20 parts by weight of blowing agent, 20 parts by weight of additives and 25 parts by weight of curing Agents are mixed to prepare phenolic resin glue. The above-mentioned high-performance phenolic resin has a viscosity of 1600cps, a gel time greater than 3 minutes, and a foaming ratio of 25 times. The foaming agent is n-pentane, the additive is silicone oil, and the curing agent is phosphoric acid.
[0025] Put the prepared high-performance phenolic resin glue into the gluing device, place the honeycomb material on the operating table, turn on the gluing device, the resin glue flows out from the mouth of the gluing device evenly, and passes through the height-fixed scraper on the device. Coat the resin evenly on the surface of the honeycomb, and then send the honeycomb int...
Embodiment 3
[0027] A preparation method for continuous height-fixed thickness phenolic foam filled honeycomb material, specifically comprising the following steps: 100 parts by weight of high-performance phenolic resin, 30 parts by weight of blowing agent, 30 parts by weight of additives and 30 parts by weight of curing Agents are mixed to prepare phenolic resin glue. The above-mentioned high-performance phenolic resin has a viscosity of 1750 cps, a gel time greater than 3 minutes, and a foaming ratio of 30 times. The foaming agent is n-pentane, the additive is Tween, and the curing agent is phosphoric acid.
[0028] Put the prepared high-performance phenolic resin glue into the gluing device, place the honeycomb material on the operating table, turn on the gluing device, the resin glue flows out from the mouth of the gluing device evenly, and passes through the height-fixed scraper on the device. Coat the resin evenly on the surface of the honeycomb, and then send the honeycomb into the ...
PUM
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com