Preparation method for environment-friendly ramie paper pulp
A kind of pulp and environmental protection technology, applied in pulp beating/refining method, beating/refining control device, non-woody plant/crop pulp, etc., can solve the problems of easy breakage and insufficient toughness of paper, and achieve less time and improve The effect of low strength and energy consumption
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Examples
Embodiment 1
[0015] Use a pulverizer to crush the dry ramie into short fibers of 30-80 mesh, put the short fibers into a container with a sealing ring to balance the water, and measure the moisture regain of the short fibers; weigh the quality of the short fibers, and calculate the fiber according to the moisture regain. Dry weight; add distilled water to the short fiber, and soak the cellulose in distilled water to fully wet the cellulose; wherein, add distilled water to the short fiber so that the mass percentage concentration of the cellulose solid in the distilled water is 3%, and the soaking time in distilled water is 20h.
[0016] Stir short fibers with a beater to make cellulose pulp; put the prepared pulp into an ultrafine refiner, the rotor and stator discs of the ultrafine refiner have gaps and grooves on the surface, set the rotor and stator The distance between the discs allows the slurry to pass through the gap between the grinding stones of the ultra-fine refiner; adjust the r...
Embodiment 2
[0021] Use a pulverizer to crush the dry ramie into short fibers of 30-80 mesh, put the short fibers into a container with a sealing ring to balance the water, and measure the moisture regain of the short fibers; weigh the quality of the short fibers, and calculate the fiber according to the moisture regain. Dry weight; add distilled water to the short fibers, and soak the cellulose in distilled water to fully wet the cellulose; wherein, add distilled water to the short fibers so that the mass percentage concentration of cellulose solids in distilled water is 5%, and the soaking time in distilled water is 40h.
[0022] Stir short fibers with a beater to make cellulose pulp; put the prepared pulp into an ultrafine refiner, the rotor and stator discs of the ultrafine refiner have gaps and grooves on the surface, set the rotor and stator The distance between the discs allows the slurry to pass through the gap between the grinding stones of the ultra-fine refiner; adjust the rotati...