A technology for wooden floors and strips, which is applied in the joining of wooden veneers, manufacturing tools, and wood processing utensils, etc., can solve problems such as insignificant effects, and achieve the effects of saving wood resources, improving floor strength, and superior economic benefits.
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Image
Examples
Embodiment 1
[0022] Embodiment 1: A kind of discarded wooden strip mosaic wooden floor, as attached figure 1 As shown, it includes a surface board 1, a finger-jointed upper board 2, a reinforced core board 3, and a bottom board 4 from top to bottom. Board 3 is formed by pasting bamboo slices 6 and wooden blocks 7 face to face. A stress groove 8 is opened at the bottom of the bottom plate 4 . The bamboo slices 6 and wooden blocks 7 are alternately arranged at intervals.
Embodiment 2
[0023] Embodiment 2: The finger-jointed upper layer board is formed by pasting and splicing wooden strips from end to end, and the reinforced core board is formed by pasting bamboo chips and wooden blocks face to face, and the adhesive used includes 30 parts of ethylene-vinyl acetate copolymer , 35 parts of polyvinyl alcohol, 10 parts of acetamide, 10 parts of crosslinking agent, 6 parts of potassium persulfate, 8 parts of stearic acid, 2 parts of fiber magnesium silicate, 2 parts of toughening agent, and 5 parts of filler. The crosslinking agent is 1 / 2 zinc oxide and 1 / 2 lead oxide, the toughening agent is polysulfide rubber, and the filler is aluminum nitride. The preparation method of the adhesive only needs to mix and stir the above components.
Embodiment 3
[0024] Embodiment 3: The adhesive comprises 40 parts of ethylene-vinyl acetate copolymer, 30 parts of polyvinyl alcohol, 30 parts of acetamide, 8 parts of crosslinking agent, 8 parts of potassium persulfate, 5 parts of stearic acid, cellulose silicic acid Magnesium 5 parts, toughening agent 3 parts, filler 10 parts. The crosslinking agent is 1 / 3 lead oxide and 2 / 3 magnesium oxide, the toughening agent is nitrile rubber, and the filler is boron nitride.