A technology for medical devices and plasticizers, applied in the field of plasticizers, can solve the problems of difficult popularization and application of common products, complicated operation and high cost, and achieve the effects of being beneficial to social economy, high technical content and good quality
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Image
Examples
Embodiment 1
[0022] A preparation method based on a plasticizer for plastic medical appliances, the specific method steps are as follows:
[0023] (1) Use waste oil produced in catering as a raw material, put it in a container and heat it to 90°C, keep it for about 30 minutes, evaporate part of the water, and filter off the foam scum on the surface;
[0024] (2) Put the waste oil in the step (1) into the reaction kettle, turn on the stirring function, control the stirring speed at 280 rpm, stir continuously for about 40 minutes, stop stirring, put into activated clay for decolorization, activated clay and waste oil The weight ratio of the mixture is 2:100; keep the temperature at 68°C, stir continuously for 12 hours, filter when the temperature drops to about 40°C, and collect the liquid oil for later use;
[0025] The semi-solid activated clay that above-mentioned filtration produces recycles and uses again;
[0026] (3) Put the liquid oil into the reaction kettle, heat up to 75°C, put i...
Embodiment 2
[0033] A preparation method based on a plasticizer for plastic medical appliances, the specific method steps are as follows:
[0034] (1) Use waste oil produced in catering as raw material, put it into a container and heat it to 70°C, keep it for about 30 minutes, evaporate part of the water, and filter off the foam scum on the surface;
[0035] (2) Put the waste oil in the step (1) into the reaction kettle, turn on the stirring function, control the stirring speed at 260 rpm, stir continuously for about 40 minutes, stop stirring, put into activated clay for decolorization, activated clay and waste oil The weight ratio of the mixture is 6:100; keep the temperature at 65°C, stir continuously for 12 hours, filter when the temperature drops to about 40°C, and collect the liquid oil for later use;
[0036] The semi-solid activated clay that above-mentioned filtration produces recycles and uses again;
[0037] (3) Put the liquid oil into the reaction kettle, heat up to 65°C, put i...