Drying technology for timber

A drying process and drying technology, applied in wood processing equipment, wood treatment, wood heating, etc., can solve the problems of unreasonable data setting, low drying efficiency, and large energy consumption, and achieve good promotion and use value, floor wood The effect of smoother surface and reduced cracking rate

Inactive Publication Date: 2017-09-08
NANTONG BOTAI ART PATTERN DESIGN CO LTD
View PDF5 Cites 1 Cited by
  • Summary
  • Abstract
  • Description
  • Claims
  • Application Information

AI Technical Summary

Problems solved by technology

[0003] The wood with a thickness of no more than 13cm is used to make the floor. The drying method in the prior art mostly adopts the kiln drying method. The air and steam in the kiln are circulated to dry the floor wood. Since the best drying standard for the floor wood cannot be grasped, various data settings are unreasonable during the drying process. There are problems such as cracking, warping, and deformation of the floor wood. At the same time, the drying efficiency of this method is not high and the energy consumption is large

Method used

the structure of the environmentally friendly knitted fabric provided by the present invention; figure 2 Flow chart of the yarn wrapping machine for environmentally friendly knitted fabrics and storage devices; image 3 Is the parameter map of the yarn covering machine
View more

Examples

Experimental program
Comparison scheme
Effect test

Embodiment 1

[0030] A drying process for floor wood, comprising the steps of:

[0031] (1) Floor pretreatment:

[0032] Select the floor wood with a thickness of 14mm, cut it according to the actual processing requirements, and then remove impurities such as sawdust for later use;

[0033] (2) First-level drying treatment of the floor:

[0034] Put the processed floor in step (1) into a drying chamber, and dry it quickly until the water content of the floor is 30-40% for later use;

[0035] (3) Secondary drying treatment of the floor:

[0036] The floors after the initial drying treatment in step (2) are stacked and stacked in layers in the drying room. Each pile is formed by stacking 20 to 30 layers of floors. Dry powder additives are filled between each floor. Horizontally stacked on the drying rack, the stacking distance between each pile is 45-50cm, the temperature in the drying room is controlled at 63-65°C, the relative humidity of the air is 55-55%, and the pressure in the drying...

the structure of the environmentally friendly knitted fabric provided by the present invention; figure 2 Flow chart of the yarn wrapping machine for environmentally friendly knitted fabrics and storage devices; image 3 Is the parameter map of the yarn covering machine
Login to View More

PUM

No PUM Login to View More

Abstract

The invention discloses a drying technology for floor timber, and belongs to the technical field of timber processing. The drying technology specifically comprises the steps of (1) processing a floor, (2) carrying out primary drying treatment on the floor, (3) carrying out secondary drying treatment on the floor, (4) carrying out third-stage drying treatment on the floor, (5) carrying out fourth-stage drying treatment on the floor, and (6) carrying out drying post-treatment on the floor. The drying technology has the advantages that the phenomena that the floor timber get deformed, cracked and bent in the drying process can be well prevented, the drying time can be shortened by 40-60%, the probability of cracking of the floor timber can be reduced by more than two times, the surface of the dried floor timber can be more smooth, and the drying technology has good popularization and application values.

Description

technical field [0001] The invention belongs to the technical field of wood processing, and in particular relates to a drying process for floor wood. Background technique [0002] Floor wood must be pretreated before it is put into use, and among them, wood drying is an important link and the most critical process in the first step; the quality of drying directly affects the utilization rate of wood and the processing of subsequent processes, directly It affects the final quality of wood products. [0003] The wood with a thickness of no more than 13cm is used to make the floor. The drying method in the prior art mostly adopts the kiln drying method, that is, the floor wood is piled up in the drying kiln, and the air in the kiln is repeatedly and alternately heated and steam is sprayed into the kiln. The air and steam in the kiln are circulated to dry the floor wood. Since the best drying standard for the floor wood cannot be grasped, various data settings are unreasonable ...

Claims

the structure of the environmentally friendly knitted fabric provided by the present invention; figure 2 Flow chart of the yarn wrapping machine for environmentally friendly knitted fabrics and storage devices; image 3 Is the parameter map of the yarn covering machine
Login to View More

Application Information

Patent Timeline
no application Login to View More
Patent Type & Authority Applications(China)
IPC IPC(8): B27K5/00
CPCB27K5/001
Inventor 陈霞
Owner NANTONG BOTAI ART PATTERN DESIGN CO LTD