Copper gold silver ore flotation collecting agent and flotation method
A collector, gold and silver technology, used in flotation, solid separation and other directions, can solve the problems of high cost and low beneficiation efficiency, and achieve the effect of improving the effect, shortening the flotation time, and reducing investment and operating costs.
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Examples
Embodiment 1
[0037] Collector Ester-205 is made from the following raw materials: N, N-diethyldithiocarbamate propionitrile 35g, diisopropyl ammonium dithiophosphate 20g, black medicine 13g, terpineol oil 30g, Ethanol 2g.
[0038] A method for flotation of copper, gold and silver ore, comprising the following steps:
[0039] Step 1, preparation of flotation pulp:
[0040] Add 500g / t of lime to the copper-gold-silver ore, mix the lime-mixed copper-gold-silver ore with water of the same quality and send it to a ball mill for grinding. The copper-gold-silver ore that is ground to a particle size of less than 0.074mm accounts for 70% of the total particle size. %, add water to the mass concentration of the pulp to 32% in the ground pulp;
[0041] Step two, flotation preparation:
[0042] Add 80g / t of butyl xanthate and 40g / t of collector ester-205 to the prepared pulp, then mix and stir for 2min in the flotation impeller at a speed of 1800 rpm for later use;
[0043] Step 3, copper, gold a...
Embodiment 2
[0048]Collector Ester-205 is made of the following raw materials: N, N-diethyldithiocarbamate propionitrile 40g, diisopropyl ammonium dithiophosphate 25g, black medicine 10g, terpineol oil 20g, Ethanol 5g.
[0049] A method for flotation of copper, gold and silver ore, comprising the following steps:
[0050] Step 1, preparation of flotation pulp:
[0051] Add 1000g / t of lime to the copper-gold-silver ore, mix the lime-mixed copper-gold-silver ore with water of the same quality and send it to a ball mill for grinding. The copper-gold-silver ore that is ground to a particle size of less than 0.074mm accounts for 75% of the total particle size. %, add water to the mass concentration of the pulp to be 33% in the ground pulp;
[0052] Step two, flotation preparation:
[0053] Add butyl xanthate 90g / t and collector ester-205 45g / t to the prepared pulp, then mix and stir for 2min in the flotation impeller at a speed of 1850 rpm for later use;
[0054] Step 3, copper, gold and si...
Embodiment 3
[0059] Collector Ester-205 is made from the following raw materials: N, N-diethyldithiocarbamate propionitrile 30g, diisopropyl ammonium dithiophosphate 22g, black medicine 15g, terpineol oil 30g, Ethanol 3g.
[0060] A method for flotation of copper, gold and silver ore, comprising the following steps:
[0061] Step 1, preparation of flotation pulp:
[0062] Add 1000g / t of lime to the copper-gold-silver ore, mix the lime-mixed copper-gold-silver ore with water of the same quality and send it to a ball mill for grinding. The copper-gold-silver ore that is ground to a particle size of less than 0.074mm accounts for 75% of the total particle size. %, add water to the mass concentration of the pulp to 34% in the ground pulp;
[0063] Step two, flotation preparation:
[0064] Add 100 g / t of butyl xanthate and 50 g / t of collector ester-205 to the prepared pulp, then mix and stir for 3 min in the flotation impeller at a speed of 1900 rpm for later use;
[0065] Step 3, copper, g...
PUM
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com