Flat welding method for trihedral drill pipe
A welding method and drill pipe technology, applied in welding equipment, non-electric welding equipment, metal processing equipment, etc., can solve the problems of easy fracture, enterprise production, operation cost and economic benefit impact, poor coaxiality of male and female joints, etc. , to ensure the coaxiality, solve the phenomenon of backwater, and eliminate the effect of stomata
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Examples
Embodiment 1
[0020] A method for welding a triangular drill pipe with flat ends, the welding method comprising the steps of:
[0021] Step 1: Pre-welding treatment: remove scale, rust, oily impurities, moisture, etc. on the surface of the weldment;
[0022] Step 2: Body shaping: Shaping each part of the weldment for use;
[0023] Step 3: preheating before welding: preheat the weldment before welding, preheat each weldment at the same time, and monitor the temperature;
[0024] Step 4: Friction welding: Friction welding parameters are: primary friction pressure 2MPa, primary friction time 5s; secondary friction pressure 4.5MPa, secondary displacement 5mm; upsetting pressure 10 MPa, upsetting pressure holding time 9s;
[0025] Step 5: Heat treatment of the weld seam: adopt the treatment process of quenching and high temperature tempering to obtain tempered sorbite;
[0026] Step 6: Post-weld inspection: Ultrasonic inspection is performed on the weld joint of the triangular drill pipe after...
Embodiment 2
[0029] A method for welding a triangular drill pipe with flat ends, the welding method comprising the steps of:
[0030] Step 1: Pre-welding treatment: remove scale, rust, oily impurities, moisture, etc. on the surface of the weldment;
[0031] Step 2: Body shaping: Shaping each part of the weldment for use;
[0032] Step 3: preheating before welding: preheat the weldment before welding, preheat each weldment at the same time, and monitor the temperature;
[0033] Step 4: Friction welding: Friction welding parameters are: primary friction pressure 2.5MPa, primary friction time 5s; secondary friction pressure 5MPa, secondary displacement 5mm; upsetting pressure 10 MPa, upsetting pressure holding time 9s;
[0034] Step 5: Heat treatment of the weld seam: adopt the treatment process of quenching and high temperature tempering to obtain tempered sorbite;
[0035] Step 6: Post-weld inspection: Ultrasonic inspection is performed on the weld joint of the triangular drill pipe after...
PUM
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com