A production process, pearl cotton technology, applied in the production process of EPE pearl cotton, can solve the problems of poor pressure resistance and cushioning performance, insignificant energy saving and environmental protection effects, easy deformation of EPE pearl cotton, etc., to achieve pressure resistance and Good cushioning performance, non-deformable plasticity, and strong toughness
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Examples
Embodiment 1
[0026] 1) Mix and stir, mix the LDPE granules, nucleating agent and antistatic agent evenly in proportion, the base material occupies 65 parts of the total preparation materials, the nucleating agent occupies 8 parts of the total preparation materials, and the antistatic agent occupies the total preparation materials of 8 servings.
[0027] 2) Heating and melting, sending the uniformly mixed raw materials into the foaming machine at a pressure of 10 MPa, the raw materials are sent into the foaming machine, and firstly subjected to heat treatment at a heating temperature of 160° C., so that the raw material mixture melts to a liquid state at a constant temperature, The constant temperature is 175°C.
[0028] 3) Foaming, the medium-high temperature liquid raw material mixture in step 2) is foamed into a porous structure under the catalytic action of monoglyceride and butane agent, and the temperature of the raw material is lowered to 120°C in the molding heating section, and the...
Embodiment 2
[0034] 1) Mix and stir, mix the LDPE colloidal particles, nucleating agent and antistatic agent in proportion evenly, the base material occupies 67 parts of the total preparation materials, the nucleating agent occupies 9 parts of the total preparation materials, and the antistatic agent occupies the total preparation materials of 9 servings.
[0035] 2) Heating and melting, sending the uniformly mixed raw materials into the foaming machine at a pressure of 15 MPa, the raw materials are sent into the foaming machine, and firstly subjected to heat treatment, the heating temperature is 170°C, so that the raw material mixture is melted to a liquid state at a constant temperature, The constant temperature is 180°C.
[0036] 3) Foaming, the medium-high temperature liquid raw material mixture in step 2) is foamed into a porous structure under the catalytic action of monoglyceride and butane agent, and the temperature of the raw material is lowered to 140°C in the molding heating sec...
PUM
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com