A fragrance and table technology, applied in disinfection, deodorization and other directions, can solve the problems of great influence on lower customers, long odor emission time, and pungent cleaning agent, so as to achieve no secondary pollution, improve environmental odor, and eliminate Effects of side effects
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Image
Examples
specific Embodiment 1
[0024] Specific embodiment 1: a kind of nontoxic deodorant that is sprayed on the dining table, comprises the following parts by weight and is prepared from: comprising mixed type epoxy resin-10 parts, liquid polysulfide rubber 20 parts, polyglucosamine is (1 -4) 13 parts of 2-amino-B-D glucose, 30 parts of ethanol, 5 parts of nano titanium dioxide, 20 parts of mixed epoxy resin, 15 parts of activated carbon, 15 parts of synthetic zeolite, 15 parts of diatomaceous earth, activated alumina powder 15 parts, 3 parts of polyvinyl acetate emulsion.
[0025] The preparation method comprises the steps of adding mixed epoxy resin 1 and liquid polysulfide rubber into a stirrer and stirring for 10 minutes to obtain mixed solution 1;
[0026] Pour polyglucosamine (1-4)-2-amino-B-D glucose, ethanol, and nano-titanium dioxide into agitator 2, and stir for 10 minutes to obtain mixed solution 2;
[0027] After mixing the mixed solution 1 and the mixed solution 2, filter them, put them into ...
specific Embodiment 2
[0042] Specific embodiment 2: a kind of nontoxic deodorant that is sprayed on the dining table, comprises the following parts by weight and is prepared from: comprise mixed type epoxy resin-40 parts, liquid polysulfide rubber 30 parts, polyglucosamine is (1 -4) 15 parts of 2-amino-B-D glucose, 50 parts of ethanol, 6 parts of nano titanium dioxide, 40 parts of mixed epoxy resin, 25 parts of activated carbon, 20 parts of synthetic zeolite, 20 parts of diatomaceous earth, activated alumina powder 20 parts, 10 parts of polyvinyl acetate emulsion.
[0043] The preparation method comprises the steps of adding mixed epoxy resin 1 and liquid polysulfide rubber into a stirrer and stirring for 10 minutes to obtain mixed solution 1;
[0044] Pour polyglucosamine (1-4)-2-amino-B-D glucose, ethanol, and nano-titanium dioxide into agitator 2, and stir for 10 minutes to obtain mixed solution 2;
[0045] After mixing the mixed solution 1 and the mixed solution 2, filter them, put them into a...