Processing technology of explosion-proof glass cover used for charging cabinet
An explosion-proof glass and processing technology, applied in glass/slag layered products, applications, household appliances, etc., can solve problems such as fire hazards, achieve good explosion-proof and fire resistance, improve fire resistance, and improve quality.
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Examples
Embodiment 1
[0035] The processing technology of the explosion-proof glass cover for the charging cabinet of the present embodiment comprises the following steps:
[0036] (1) Making composite material frame, the specific steps are as follows:
[0037] a. Ingredients: The mass percentage of the composite material frame is: styrene: 2.23%, styrene-butadiene rubber: 4.21%, EPDM rubber: 6.45%, epoxy resin: 12.45%, magnesium chloride: 1.33%, zinc oxide: 2.33%, glass fiber: 1.55%, release agent: 1.45%, ultraviolet absorber: 2.32%, and the balance is phenolic resin;
[0038] b. Pulverize the raw materials of the composite material frame after batching with a pulverizer;
[0039] c. Drying: Drying the pulverized raw materials of the composite frame, the drying temperature is 60-90°C, and the drying time is 7-9 hours;
[0040] d, injecting the raw material of the dried composite material frame into a composite material frame;
[0041] e. The composite material frame is vulcanized in a steam vul...
Embodiment 2
[0055] The processing technology of the explosion-proof glass cover for the charging cabinet of the present embodiment comprises the following steps:
[0056] (1) Making composite material frame, the specific steps are as follows:
[0057] a. Ingredients: The mass percentage of the composite material frame is: styrene: 3.67%, styrene-butadiene rubber: 5.45%, EPDM rubber: 7.25%, epoxy resin: 12.89%, magnesium chloride: 1.56%, zinc oxide: 2.54%, glass fiber: 2.16%, release agent: 1.78%, ultraviolet absorber: 2.56%, and the balance is phenolic resin;
[0058] b. Pulverize the raw materials of the composite material frame after batching with a pulverizer;
[0059] c. Drying: Drying the pulverized raw materials of the composite frame, the drying temperature is 60-90°C, and the drying time is 7-9 hours;
[0060] d, injecting the raw material of the dried composite material frame into a composite material frame;
[0061] e. The composite material frame is vulcanized in a steam vul...
PUM
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com