No-solvent double-ingredient polyurethane track material and preparation method thereof
A two-component polyurethane, solvent-free technology, applied in the direction of roads, roads, pavements, etc., can solve the problems of overall product performance gap, lack of independent intellectual property rights, lagging development, etc., to achieve improved environmental performance, good mechanical properties, and low VOC Effect
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Image
Examples
preparation example Construction
[0050] The preparation process of embodiment 1-4 is:
[0051] Preparation of component A: Add polyether polyol and plasticizer into a reaction kettle equipped with a thermometer, stirring and vacuum system, stir and raise the temperature to 100-115°C, dehydrate under 0.06MPa vacuum to the moisture content of the material in the kettle Below 0.05% by mass, cool down to 60°C, add MDI, heat up to 70-80°C and keep warm to react until the NCO value in the system reaches 7.5%, put it into a nitrogen-protected airtight container for storage after cooling down;
[0052] Preparation of component B: Add polyether polyol and crosslinking agent, pigments, fillers and additives into the dehydration kettle, stir and heat up to 100-110°C, and dehydrate under 0.06MPa vacuum until the moisture content of the material is 0.05 mass % or less; then cool down to 60°C, add 0.05-1 special additives to disperse for 1 hour, filter and pack.
[0053] Preparation of the test piece: According to the NCO...
PUM
| Property | Measurement | Unit |
|---|---|---|
| hydroxyl value | aaaaa | aaaaa |
Abstract
Description
Claims
Application Information
Login to View More 