Building color sand, method for preparing same and application of building color sand
A technology for construction and colored sand, applied in the field of construction colored sand and preparation, can solve the problem of high cost
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Examples
preparation example Construction
[0027] Aiming at the new changes and demands of building energy-saving external wall structure, the present invention provides a kind of colored sand for building, its preparation method and its application, which uses the raw material of colored sand containing waste glass to carry out all-inorganic high-temperature sintering to prepare colored sand, which can realize Green recycling of waste glass; the prepared colored sand is mainly used for building exterior walls, and can also be used for building colored tiles and interior decoration.
[0028] The first purpose of the present invention is to provide a kind of colored sand for construction:
[0029] Colored sand is sintered from colored sand raw materials, which include: batch materials, adhesives and quartz sand; of which:
[0030] The batching material of the present invention includes waste glass, borax, antimony white and inorganic colorant, preferably only the above four components constitute the batching material; t...
Embodiment 1
[0051] The invention provides a kind of colored sand for building and its preparation method. It is prepared according to the mass ratio of waste glass to borax of 80:20, adding 7% chrome green and 2% antimony white, and mixing evenly to form a batch material. The mass fraction of the batch material accounts for 6% of the mass fraction of the quartz sand, and a 150,000-viscosity hydroxypropyl methylcellulose ether aqueous solution with a solid content of 0.1% is added. Put it in a 740°C kiln and bake it into green colored sand.
Embodiment 2
[0053] The invention provides a kind of colored sand for construction and its preparation method. It is prepared according to the mass ratio of waste glass to borax of 90:10, adding 1% cobalt oxide and 5% antimony white, and mixing evenly to become a batch material; the mass of the batch material accounts for the mass of quartz sand 3% of the fraction, add a 150,000-viscosity hydroxypropyl methylcellulose ether aqueous solution with a solid content of 0.3%. It is advisable to firmly grasp the critical point of agglomeration after the amount of aqueous solution is added and stirred. Put it in a kiln at 880°C and bake it into blue colored sand.
PUM
Property | Measurement | Unit |
---|---|---|
Particle size | aaaaa | aaaaa |
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com