A technology of soil loosening and conditioner, applied in the field of soil conditioning, can solve problems such as shortage, difficulty in loosening the soil of Chinese torreya, and roots that are easy to cause insect damage and nutrition, and achieve the effects of increasing fertilizer retention, improving mixing effect, and increasing photosynthesis
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Image
Examples
Embodiment 1
[0024] The method embodiment of preparing above-mentioned soil loosening and carbon-increasing conditioner, comprises the following steps:
[0025] According to the calculation of preparing a total weight of 100 kg of soil loosening and carbon-increasing conditioner, weigh 5 kg of millet straw and place it in a carbonization furnace, slowly heat it to 500 °C in a relatively sealed state, and keep it for 2 hours before stopping heating , and immediately after stopping the heating, take out the carbonized straw and put it into the mixing device, then weigh 15kg of river sand, 10kg of rice bran and 5kg of sawdust and put them into the mixing device to fully stir with the carbonized straw for 3 hours, then let it stand 20 days, the mixing device is in a closed state when standing still;
[0026] Weigh 30kg of poultry manure and 20kg of cake fertilizer, then put the weighed poultry manure and cake fertilizer into a stirring device and mix them for 26 minutes, take them out after st...
Embodiment 2
[0032] The method embodiment of preparing above-mentioned soil loosening and carbon-increasing conditioner, comprises the following steps:
[0033] According to the calculation of preparing 100 kg of soil loosening and carbon-increasing conditioner in total, weigh 7 kg of millet straw and place it in a carbonization furnace, heat it slowly to 510 °C in a relatively sealed state, and keep it for 2.5 hours before stopping heating , and immediately after stopping the heating, take out the carbonized straw and put it into the mixing device, then weigh 13kg of river sand, 5kg of rice bran and 14kg of sawdust and put them into the mixing device to fully stir with the carbonized straw for 4 hours, then let it stand 25 days, the mixing device is in a closed state when standing still;
[0034] Weigh 20kg of poultry manure and 23kg of cake fertilizer, then put the weighed poultry manure and cake fertilizer into a stirring device and mix them for 32 minutes, take them out after stirring ...
Embodiment 3
[0040] The method embodiment of preparing above-mentioned soil loosening and carbon-increasing conditioner, comprises the following steps:
[0041] According to the calculation of preparing a total weight of 100 kg of soil loosening and carbon-increasing conditioner, weigh 10 kg of millet straw and place it in a carbonization furnace, slowly heat it to 530°C in a relatively sealed state, and keep it for 3 hours before stopping heating , and immediately after stopping the heating, take out the carbonized straw and put it into the mixing device, then weigh 16kg of river sand, 5kg of rice bran and 7kg of sawdust and put them into the mixing device to fully stir with the carbonized straw for 5 hours, then let it stand 30 days, the mixing device is in a closed state when standing still;
[0042] Weigh 25kg of poultry manure and 30kg of cake fertilizer, then place the weighed poultry manure and cake fertilizer into a stirring device and mix them for 37 minutes, take them out after s...