Sludge curing agent and preparation method thereof
A technology of sludge solidification agent and coagulation accelerator, which is applied in chemical instruments and methods, sludge treatment, fixed/solidified sludge treatment, etc. It can solve soil and groundwater pollution, sludge with poor mechanical properties and difficult to reuse To achieve the effect of promoting sludge dehydration, loosening sludge structure and increasing adsorption effect
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Image
Examples
Embodiment 1
[0029] Embodiment 1 A kind of sludge curing agent
[0030] The sludge curing agent is composed of the following components and parts by weight: 30 parts of attapulgite, 25 parts of modified straw, 18 parts of coagulant, 10 parts of bactericide, 5 parts of phenolic resin and carboxymethyl cellulose 0.5 parts of sodium; the bactericide is composed of calcium propionate and polyquaternium salt in a weight ratio of 1:9.
[0031] The preparation method of the modified straw is as follows: take 80 parts of corn stalks, dry them at 100°C, crush them to 100 mesh, add 40% citric acid aqueous solution which is 6 times the weight of the corn stalks, heat to 100°C, and stir After 80 minutes, add 20 parts of polyacrylamide and stir for 30 minutes, dry and crush through a 200-mesh sieve to obtain the product.
[0032] The coagulant is composed of the following components and parts by weight: 40 parts of cassava flour, 8 parts of acrylic acid, and 1 part of initiator; the initiator is ammon...
Embodiment 2
[0037] Embodiment 2 A kind of sludge curing agent
[0038] The sludge curing agent is composed of the following components and parts by weight: 40 parts of attapulgite, 35 parts of modified straw, 20 parts of coagulant, 12 parts of bactericide, 8 parts of phenolic resin and carboxymethyl cellulose 1.5 parts of sodium; the bactericide is composed of calcium propionate and polyquaternium salt in a weight ratio of 2:7.
[0039] The preparation method of the modified straw is as follows: take 80 parts of corn stalks, dry them at 100°C, crush them to 120 mesh, add 40% citric acid aqueous solution which is 7 times the weight of the corn stalks, heat to 110°C, stir After 80 minutes, add 20 parts of polyacrylamide and stir for 30 minutes, dry and crush through a 200-mesh sieve to obtain the product.
[0040] The coagulant is composed of the following components and parts by weight: 50 parts of cassava flour, 12 parts of acrylic acid, and 3 parts of initiator; the initiator is ammoniu...
Embodiment 3
[0045] Embodiment 3 a kind of sludge curing agent
[0046] The sludge curing agent is composed of the following components and parts by weight: 50 parts of attapulgite, 40 parts of modified straw, 28 parts of coagulant, 15 parts of bactericide, 10 parts of phenolic resin and carboxymethyl cellulose 2.0 parts of sodium; the bactericide is composed of calcium propionate and polyquaternium salt in a weight ratio of 3:4.
[0047] The preparation method of the modified stalks is as follows: take 80 parts of corn stalks, dry them at 100°C, crush them to 130 mesh, add 40% citric acid aqueous solution which is 8 times the weight of the corn stalks, heat to 120°C, stir After 80 minutes, add 20 parts of polyacrylamide and stir for 30 minutes, dry and crush through a 200-mesh sieve to obtain the product.
[0048] The coagulant includes the following components and parts by weight: 60 parts of cassava flour, 18 parts of acrylic acid, and 5 parts of initiator; the initiator is ammonium pe...
PUM
| Property | Measurement | Unit |
|---|---|---|
| compressive strength | aaaaa | aaaaa |
| compressive strength | aaaaa | aaaaa |