A composite pipe for home improvement
A composite pipe and home improvement technology, applied in the field of pipes, can solve the problems of easy aging service life, no protective layer, not scratch resistance, etc., and achieve the effect of low thermal conductivity, good thermal insulation effect, and improved thermal insulation performance.
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Image
Examples
Embodiment 1
[0029] The home decoration composite pipe of this embodiment comprises a hollow pipe body 1 of PPR material, an insulation layer 2, a PIR layer and a protective layer 3 of a galvanized sheet arranged in sequence from the inside to the outside, and the insulation layer 2 includes the following parts by weight Preparation raw materials: 52 parts of diatomite, 12 parts of vermiculite powder, 23 parts of water-based polyurethane resin, 5 parts of magnesium oxide, 5 parts of carboxymethyl cellulose, 3 parts of 11 μm hollow glass microspheres and foaming agent (sodium bicarbonate and citric acid in a weight ratio of 1:1) 5 parts. The thickness ratio of the hollow pipe body, insulation layer, protective layer and PIR layer is 5:2:6:2. The particle size of diatomite is controlled to be 1000 mesh; the particle size of magnesium oxide, carboxymethyl cellulose and foaming agent are all controlled to be 800 mesh; the particle size of vermiculite powder is all controlled to be 150 mesh.
...
Embodiment 2
[0035] Only the "insulation layer" includes the following preparation raw materials in parts by weight: 58 parts of diatomite, 15 parts of vermiculite powder, 30 parts of water-based polyurethane resin, 8 parts of magnesium oxide, 8 parts of carboxymethyl cellulose, and 7 parts of hollow glass microspheres of 17 μm 8 parts and foaming agent (the mixture of sodium bicarbonate and citric acid mixed in a weight ratio of 1:1). The ratio of the thickness of the hollow tube body, insulation layer, protective layer and PIR layer is 7:5:8 : 3." Different from Example 1, others are the same as Example 1.
Embodiment 3
[0037] Only "the insulation layer includes the following preparation raw materials in parts by weight: 55 parts of diatomite, 14 parts of vermiculite powder, 26 parts of water-based polyurethane resin, 6 parts of magnesium oxide, 6 parts of carboxymethyl cellulose, 6 parts of hollow glass microspheres of 16 μm 6 parts and foaming agent (the mixture of sodium bicarbonate and citric acid mixed in a weight ratio of 1:1). The ratio of the thickness of the hollow tube body, insulation layer, protective layer and PIR layer is 6:3:7 : 2." Different from Example 1, others are the same as Example 1.
PUM
| Property | Measurement | Unit |
|---|---|---|
| particle size | aaaaa | aaaaa |
| particle diameter | aaaaa | aaaaa |
| size | aaaaa | aaaaa |