Enhanced anti-skid sole and anti-skid shoe
An enhanced, non-slip technology, applied in the field of shoes, can solve the problems of easy slipping, accidental slipping on the ground, limited effect, etc., and achieve the effects of increasing wet friction coefficient, dry friction coefficient and strong adhesion.
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Examples
Embodiment 1
[0038] Including anti-skid sole, described anti-skid sole is made up of the material of following parts by weight:
[0039] 80 parts of natural rubber;
[0040] 10 parts of styrene-butadiene rubber;
[0041] Accelerator 1 part;
[0042] Antioxidant 0.1 part;
[0043] Active agent 2.5 parts;
[0044] 2 parts sulfur;
[0045] 5 parts of modified zirconia;
[0046] Activated sepiolite 1 part.
[0047] The preparation method of the modified zirconia comprises the following steps:
[0048] Step 1: Mix 10 parts by weight of ethanol, 100 parts by weight of vinyltrimethoxysilane and 10 parts by weight of deionized water, and add 1-10 parts by weight of hydrochloric acid solution dropwise to adjust the pH of the mixed solution to 5, The speed is 300 rpm, and the stirring time is 2 hours;
[0049] Step 2: Under the protection of nitrogen, add 10 parts by weight of zirconia and 1 part by weight of the above-mentioned mixed solution to 100 parts by weight of toluene solution and s...
Embodiment 2
[0055] Including anti-skid sole, described anti-skid sole is made up of the material of following parts by weight:
[0056] 100 parts of natural rubber;
[0057] 50 parts of styrene-butadiene rubber;
[0058] Accelerator 4 parts;
[0059] 0.5 part of antioxidant;
[0060] Active agent 4.5 parts;
[0061] 10 parts of sulfur;
[0062] 20 parts of modified zirconia;
[0063] Activated sepiolite 10 parts.
[0064] The preparation method of the modified zirconia comprises the following steps:
[0065]Step 1: Mix 100 parts by weight of ethanol, 800 parts by weight of vinyltrimethoxysilane and 100 parts by weight of deionized water, and dropwise add 10 parts by weight of hydrochloric acid solution to adjust the pH of the mixed solution to 5, at a speed of 300 rpm, stirring time 16 hours;
[0066] Step 2: Under the protection of nitrogen, add 200 parts by weight of zirconia and 20 parts by weight of the above-mentioned mixed solution to 2000 parts by weight of toluene solution...
PUM
Login to View More Abstract
Description
Claims
Application Information
Login to View More - R&D
- Intellectual Property
- Life Sciences
- Materials
- Tech Scout
- Unparalleled Data Quality
- Higher Quality Content
- 60% Fewer Hallucinations