A kind of resin ribbon and thermal transfer printing structure
A technology of resin carbon and transfer printing layer, which is applied in printing, ink ribbon, inking device, etc. It can solve the problems of easy fading, low toner transfer printing fastness, and difficulty in guaranteeing the service life of printing effect, etc., to extend the duration , Applicable to a wide range of effects
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Image
Examples
Embodiment 1-8
[0034] The preferred formulation components and parts by mass of each embodiment, wherein the tackifying resin is mixed with 4:1 by 75% degree of hydrogenation C9 petroleum resin and fully hydrogenated rosin, as shown in table 1 below:
[0035]
[0036] Test Methods
[0037] The colloid obtained by the raw material proportioning of each present embodiment 1-8 is detected using the following method:
[0038] 1. Viscosity value, put 500ml of the pre-melted sol layer sample into the drum of the viscometer, then measure the temperature (130±2°C) and keep it for 5min, let the rotor rotate for 30-60s, and take a reading.
[0039] 2. The curing time refers to scraping the sample of the sol layer on a PE board, and then bonding another PE board to it, counting from the completion of the bonding, and peeling off from one end until the PE board is damaged When it appears, it is considered that the sol layer sample has been cured, and the recorded time is the curing time of the sol l...
Embodiment 9-16
[0044] In the preferred formula obtained by the above experiment, a new augmentation component is added, and its specific mass parts are shown in Table 3 below:
[0045]
[0046] Test Methods
[0047] The colloid obtained by the raw material ratio of each embodiment 9-16 is detected using the following method:
[0048] 1. Viscosity value, put 500ml of the pre-melted sol layer sample into the drum of the viscometer, then measure the temperature (130±2°C) and keep it for 5min, let the rotor rotate for 30-60s, and take a reading.
[0049] 2. Resistance to yellowing. There are several reasons for the yellowing of the sol layer sample, including light, weathering, and oxidation reactions. These sol layer samples were coated on PE boards, placed at the same tuyere, and continuously illuminated until yellowing occurred.
[0050] 3. The curing time refers to scraping the sample of the sol layer on a PE board, and then bonding another PE board to it, counting from the completion o...
PUM
| Property | Measurement | Unit |
|---|---|---|
| melting point | aaaaa | aaaaa |
Abstract
Description
Claims
Application Information
Login to View More - R&D
- Intellectual Property
- Life Sciences
- Materials
- Tech Scout
- Unparalleled Data Quality
- Higher Quality Content
- 60% Fewer Hallucinations
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2025 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com