A kind of bamboo desugar method and its application
A bamboo and sugar-removing technology, applied in the direction of wood impregnation, impregnated wood, wood processing equipment, etc., can solve the problems of limited application range, difficult treatment, dark color, etc., to improve anti-corrosion and anti-mildew performance, increase processing added value, The effect of simple process
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Image
Examples
Embodiment 1
[0050] Embodiment 1 of the present invention provides a kind of bamboo wood desugaring method, comprises the following steps:
[0051] (1) Bamboo pretreatment: After the bamboo is rolled, it is set aside;
[0052] (2) Desugar treatment: immerse the bamboo obtained in step (1) in water, add solid alkali, and treat for 1 hour.
[0053] In step (2), the solid base is magnesium oxide.
[0054] In step (2), the added amount of the solid alkali is 0.2% of the bamboo mass.
[0055] In step (2), the mass ratio of the bamboo to water is 1:4.
[0056]In step (2), the treatment temperature is 160°C.
[0057] In step (2), the treatment pressure is 0.6MPa.
[0058] Embodiment 1 of the present invention also provides an application of the method for desugaring bamboo as described above, which is used for desugaring bamboo to produce heavy bamboo boards and by-products suitable for outdoor use.
Embodiment 2
[0060] Embodiment 2 of the present invention provides a kind of bamboo wood desugaring method, comprises the following steps:
[0061] (1) Bamboo pretreatment: After the bamboo is rolled, it is set aside;
[0062] (2) Desugar treatment: immerse the bamboo obtained in step (1) in water, add solid alkali, and treat for 1 hour.
[0063] In step (2), the solid base is magnesium hydroxide.
[0064] In step (2), the added amount of the solid alkali is 0.2% of the bamboo mass.
[0065] In step (2), the mass ratio of the bamboo to water is 1:4.
[0066] In step (2), the treatment temperature is 160°C.
[0067] In step (2), the treatment pressure is 0.6MPa.
[0068] Embodiment 2 of the present invention also provides an application of the method for desugaring bamboo as described above, which is used for desugaring bamboo to produce heavy bamboo boards and by-products suitable for outdoor use.
Embodiment 3
[0070] Embodiment 3 of the present invention provides a kind of bamboo desugaring method, comprises the following steps:
[0071] (1) Bamboo pretreatment: After the bamboo is rolled, it is set aside;
[0072] (2) Desugar treatment: immerse the bamboo obtained in step (1) in water, add solid alkali, and treat for 1 hour.
[0073] In step (2), the solid base is magnesium carbonate.
[0074] In step (2), the added amount of the solid alkali is 0.2% of the bamboo mass.
[0075] In step (2), the mass ratio of the bamboo to water is 1:4.
[0076] In step (2), the treatment temperature is 160°C.
[0077] In step (2), the treatment pressure is 0.6 MPa.
[0078] Embodiment 3 of the present invention also provides an application of the method for desugaring bamboo as described above, which is used for desugaring bamboo to produce heavy bamboo boards and by-products suitable for outdoor use.
PUM