Mural and colored drawing cultural relic reinforcing agent with self-healing function and preparation method thereof
A self-healing and reinforcing agent technology, applied in the direction of adhesive additives, non-polymer adhesive additives, adhesive types, etc., can solve problems that affect the appearance and use of cultural relics, and cannot penetrate into cultural relics, etc., to achieve high viscosity Good bonding strength, good permeability, and the effect of ensuring the reinforcement effect
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Image
Examples
Embodiment 1
[0021] In the first step, 1.4g poly(2-ethyl-2-oxazoline) and 0.6g poly(4-vinylphenol) were fully dissolved in 5.96ml DMF, poly(2-ethyl-2-oxazole) The mass ratio of morpholine to poly(4-vinylphenol) is 7:3.
[0022] In the second step, the DMF solution of poly(2-ethyl-2-oxazoline) was added dropwise to the DMF solution of poly(4-vinylphenol) while stirring, and 0.5g of calcium chloride was added, and stirred thoroughly At least 6 hours, a light yellow transparent reinforcing agent is obtained, and the total solute concentration in the solution is 0.2097 g / mL.
Embodiment 2
[0024] In the first step, 0.85g of poly(2-ethyl-2-oxazoline) and 0.15g of poly(4-vinylphenol) are fully dissolved in 10ml DMF respectively. The mass ratio of oxazoline) to poly(4-vinylphenol) is 8.5:1.5.
[0025] In the second step, the DMF solution of poly(2-ethyl-2-oxazoline) is added dropwise to the DMF solution of poly(4-vinylphenol) while stirring, and the solution is fully stirred for at least 6 hours to obtain a colorless and transparent solution. Reinforcing agent, the solid concentration in the solution is 0.0500g / mL.
Embodiment 3
[0027] In the first step, 1.6g of poly(2-ethyl-2-oxazoline) and 0.4g of poly(4-vinylphenol) were fully dissolved in 5.96ml DMF respectively, in which, poly(2-ethyl-2- The mass ratio of oxazoline) to poly(4-vinylphenol) is 8:2.
[0028] In the second step, the DMF solution of poly(2-ethyl-2-oxazoline) was added dropwise to the DMF solution of poly(4-vinylphenol) while stirring, and the mixture was fully stirred for at least 6 hours to obtain a light yellow transparent Reinforcing agent, the solid concentration in the solution is 0.1678g / mL.
PUM
Property | Measurement | Unit |
---|---|---|
Concentration | aaaaa | aaaaa |
Concentration | aaaaa | aaaaa |
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com